J Dent Res. 1980 Jun;59(6):1022-5. doi: 10.1177/00220345800590060301.
Fluoride concentration of enamel surfaces treated with 50% H3PO4, together with high NaF contents or etched with 50% H3PO4 followed by application with a water solution of high NaF content, was examined. In addition, the degree of decalcification and the fluoride content of subsequently incubated enamel samples in acid-gel at 37 degrees C were determined. Generally, incubation highly increased the fluoride contents of the etched and fluoridated (experimental), control (etched only), and untreated (vaseline) enamel samples. An increasing demineralization effect was observed in the samples of the following order: experimental, control, and baseline. It appears does not predispose to an increased caries challenge in vitro.
研究了用50%磷酸处理的牙釉质表面的氟化物浓度,以及高氟化钠含量的情况,或者先用50%磷酸蚀刻,然后再用高氟化钠含量的水溶液处理的情况。此外,还测定了随后在37℃酸凝胶中孵育的牙釉质样品的脱钙程度和氟化物含量。一般来说,孵育显著增加了蚀刻和氟化(实验性)、对照(仅蚀刻)以及未处理(凡士林)牙釉质样品中的氟化物含量。在以下顺序的样品中观察到脱矿作用增强:实验性、对照性和基线。在体外似乎不会增加龋齿的易感性。