Barber F A, Click J N
Plano Orthopedic and Sports Medicine Center, Texas 75075.
Arthroscopy. 1992;8(4):437-41. doi: 10.1016/0749-8063(92)90004-u.
The effect of inflammatory synovial fluid upon several absorbable sutures potentially useful for arthroscopic procedures, e.g., meniscus repair and shoulder stabilization, was studied by implanting lengths of these sutures into unstable, arthritic rabbit knees and testing their breaking strength after varying time periods (up to 18 weeks). Polyglyconate (Maxon) sutures retained no significant strength at 6 weeks. Polydioxanone (PDS) sutures began to lose breaking strength at 3 weeks, retained only 40% of their original strength 6 weeks after implantation, and had no measurable strength at 9 weeks. Polycaprolactone (LTS) sutures showed a slow reduction in strength and retained approximately 90% of their original breaking strength after 18 weeks of implantation. Green braided polyester (Mersiline) sutures showed no loss of breaking strength over the testing period. Measurements of inherent viscosity were made to give an indirect indication of the decline in molecular weight of these sutures. These data paralleled the breaking strength decline in every case. The surgeon selecting an absorbable suture must consider the length of time the suture will hold the target tissue. This information should be helpful to surgeons considering an absorbable suture for procedures such as meniscus repair and shoulder stabilization.
通过将几种可能用于关节镜手术(如半月板修复和肩关节稳定术)的可吸收缝线植入不稳定的患关节炎兔膝关节,并在不同时间段(长达18周)后测试其断裂强度,研究了炎性滑液对这些缝线的影响。聚乙醇酸(Maxon)缝线在6周时已无显著强度。聚二氧杂环己酮(PDS)缝线在3周时开始丧失断裂强度,植入6周后仅保留其原始强度的40%,9周时已无可测量的强度。聚己内酯(LTS)缝线的强度缓慢下降,植入18周后仍保留其原始断裂强度的约90%。绿色编织聚酯(Mersiline)缝线在测试期间未出现断裂强度损失。通过测量特性粘度来间接表明这些缝线的分子量下降情况。这些数据在每种情况下都与断裂强度的下降情况相符。选择可吸收缝线的外科医生必须考虑缝线固定目标组织的时间长度。这些信息应有助于考虑在半月板修复和肩关节稳定术等手术中使用可吸收缝线的外科医生。