[可吸收缝线Dexon和Maxon拉伸强度的比较评估。实验研究]

[Comparative evaluation of tensile strength of absorbable threads Dexon and Maxon. Experimental studies].

作者信息

Kulak Z, Deja A, Tuszewski M

机构信息

Klinika Chirurgii Ogólnej i Gastroenterologicznej Instytutu Chirurgii, Akademii Medycznej w Poznaniu.

出版信息

Polim Med. 1991;21(1-2):43-8.

PMID:1667692
Abstract

This paper submits strength tests on Dexon and Maxon resorbable sutures at the knot and without a knot, the breaking resulting from hydrolysis. The tests were performed on rats, by comparing Maxon monofilament suture with Dexon woven suture. The dissections were done 3, 7, 21 and 42 days after the implantation. What we found out was a remarkably slower process of strength loss displayed by Maxon sutures in time after the implantation. After 21 days, Dexon sutures displayed a minimal strength value, whereas Maxon sutures still retained ca 60% of the initial properties.

摘要

本文提交了关于 Dexon 和 Maxon 可吸收缝线在有结和无结情况下的强度测试,测试其因水解导致的断裂情况。测试在大鼠身上进行,将 Maxon 单丝缝线与 Dexon 编织缝线进行比较。在植入后 3、7、21 和 42 天进行解剖。我们发现,Maxon 缝线在植入后的时间里强度损失过程明显较慢。21 天后,Dexon 缝线显示出最小强度值,而 Maxon 缝线仍保留约 60%的初始性能。

文献检索

告别复杂PubMed语法,用中文像聊天一样搜索,搜遍4000万医学文献。AI智能推荐,让科研检索更轻松。

立即免费搜索

文件翻译

保留排版,准确专业,支持PDF/Word/PPT等文件格式,支持 12+语言互译。

免费翻译文档

深度研究

AI帮你快速写综述,25分钟生成高质量综述,智能提取关键信息,辅助科研写作。

立即免费体验