Shahdad Shakeel A, McCabe John F, Wassell Robert W
Restorative Dentistry, The Royal London Dental Hospital, New Road, London, UK.
J Mater Sci Mater Med. 2007 Aug;18(8):1599-603. doi: 10.1007/s10856-007-3043-4. Epub 2007 May 5.
The effect of various food-simulating solvents on the hardness of denture teeth after varying storage times, using a Martens hardness test was determined. Martens hardness (HM) was assessed at baseline and during storage up to 1 month in distilled water (DW), peppermint oil (PO), heptane (HT) and 75% ethanol (ET) for four commercially-available denture teeth; Vivodent (VIV), Double-cross-linked Postaris (DCL), Orthosit (ORT), Candulor porcelain (POR) and two polymer based experimental denture teeth: Experimental 1 (EXP1); a hybrid nanocomposite with two different sized silanated filler particles and Experimental 2 (EXP2); containing an organic copolymer based upon urethanedimethacrylate and polymethyl methacrylate. Hardness [mean (sd)] at baseline was: VIV 142 (1), DCL 142 (1), ORT 209 (9), POR 2926 (101), EXP1 285 (11), and EXP2 146 (12). One-way ANOVA using Tukey's test on polymer-based materials showed that the hardness values of ORT and EXP1 were significantly higher than those of VIV, DCL and EXP2 (P < 0.05). Moreover, EXP1 had a significantly higher hardness value than ORT (P < 0.05). Except for EXP1, all polymer based materials showed a significant drop in hardness after storage in ET (P < 0.05). Specimens stored in water, heptane and peppermint oil showed minor fluctuations in hardness, which were not statistically significant.
使用马氏硬度测试法,测定了不同储存时间后,各种食品模拟溶剂对义齿牙齿硬度的影响。对四种市售义齿牙齿(Vivodent(VIV)、双交联Postaris(DCL)、Orthosit(ORT)、Candulor瓷(POR))以及两种聚合物基实验性义齿牙齿(实验1(EXP1):一种含有两种不同尺寸硅烷化填料颗粒的混合纳米复合材料;实验2(EXP2):含有一种基于聚氨酯二甲基丙烯酸酯和聚甲基丙烯酸甲酯的有机共聚物),在基线时以及在蒸馏水(DW)、薄荷油(PO)、庚烷(HT)和75%乙醇(ET)中储存长达1个月的过程中,评估其马氏硬度(HM)。基线时的硬度[平均值(标准差)]为:VIV 142(1)、DCL 142(1)、ORT 209(9)、POR 2926(101)、EXP1 285(11)、EXP2 146(12)。对聚合物基材料进行的单向方差分析(采用Tukey检验)表明,ORT和EXP1的硬度值显著高于VIV、DCL和EXP2(P<0.05)。此外,EXP1的硬度值显著高于ORT(P<0.05)。除EXP1外,所有聚合物基材料在ET中储存后硬度均显著下降(P<0.05)。储存在水、庚烷和薄荷油中的试样硬度有微小波动,但无统计学意义。