Durkan Rukiye, Ozel Mehmet Birol, Bağiş Bora, Usanmaz Ali
Department of Prosthodontics, Faculty of Dentistry, Karadeniz Technical University, Trabzon, Turkey.
Dent Mater J. 2008 Jul;27(4):640-2.
The aim of this study was to determine the effect of autoclave polymerization on the transverse strength of denture base polymers. To this end, 30 rectangular test specimens were fabricated of two heat-polymerized denture base polymers. The test groups were: (I) control, i.e., conventional water bath to polymerize resins by heat at 100 degrees C for 30 minutes; (II) autoclave polymerization at 60 degrees C for 30 minutes followed by 130 degrees C for 10 minutes; and (III) autoclave polymerization at 60 degrees C for 30 minutes followed by 130 degrees C for 20 minutes. The specimens were tested with three-point bending test at a crosshead speed of 5 mm/min. It was revealed that the transverse strength of specimens increased with statistical significance when the autoclave was used for polymerization.
本研究的目的是确定高压釜聚合对义齿基托聚合物横向强度的影响。为此,用两种热聚合义齿基托聚合物制作了30个矩形测试样本。测试组如下:(I)对照组,即通过在100摄氏度下加热30分钟,采用传统水浴法聚合树脂;(II)在60摄氏度下高压釜聚合30分钟,然后在130摄氏度下聚合10分钟;以及(III)在60摄氏度下高压釜聚合30分钟,然后在130摄氏度下聚合20分钟。以5毫米/分钟的十字头速度对样本进行三点弯曲试验。结果显示,当使用高压釜进行聚合时,样本的横向强度有统计学意义的增加。