Electrophoretic deposition of silicon-substituted hydroxyapatite/poly(epsilon-caprolactone) composite coatings.

作者信息

Xiao Xiufeng, Liu Rongfang, Tang Xiaolian

机构信息

College of Chemistry and Materials Science, Fujian Normal University, Fuzhou, 350007, China.

出版信息

J Mater Sci Mater Med. 2009 Mar;20(3):691-7. doi: 10.1007/s10856-008-3619-7. Epub 2008 Oct 24.

Abstract

Silicon-substituted hydroxyapatite/poly(epsilon-caprolactone) composite coatings were prepared on titanium substrate by electrophoretic deposition in n-butanol and chloroform mixture. The effect of the concentration of poly(epsilon-caprolactone) in suspension on the morphology and the microstructure of coatings were investigated, furthermore, the thermal behavior and in vitro bioactivity were also investigated. The results show that the coarse and accidented silicon-substituted hydroxyapatite/poly(epsilon-caprolactone) composite coatings were obtained by electrophoretic deposition when the concentration of poly(epsilon-caprolactone) in suspension was 6-16 g/l. The adsorption of poly(epsilon-caprolactone) on the surface of Si-HA particles hinders the electrophoretic deposition of Si-HA. The shear-testing experiments indicated that the addition of poly(epsilon-caprolactone) in suspension is in favor of improving the bonding strength of the coatings. After immersion in simulated body fluid for 8 days, silicon-substituted hydroxyapatite/poly(epsilon-caprolactone) composite coatings have the ability to induce the bone-like apatite formation.

摘要

通过在正丁醇和氯仿混合物中进行电泳沉积,在钛基底上制备了硅取代羟基磷灰石/聚(ε-己内酯)复合涂层。研究了悬浮液中聚(ε-己内酯)浓度对涂层形貌和微观结构的影响,此外,还研究了其热行为和体外生物活性。结果表明,当悬浮液中聚(ε-己内酯)浓度为6-16 g/L时,通过电泳沉积可获得粗糙且凹凸不平的硅取代羟基磷灰石/聚(ε-己内酯)复合涂层。聚(ε-己内酯)在Si-HA颗粒表面的吸附阻碍了Si-HA的电泳沉积。剪切试验表明,在悬浮液中添加聚(ε-己内酯)有利于提高涂层的结合强度。在模拟体液中浸泡8天后,硅取代羟基磷灰石/聚(ε-己内酯)复合涂层具有诱导类骨磷灰石形成的能力。