Department of Prosthodontics, School of Dentistry, Johann Wolfgang Goethe University, Theodor-Stern-Kai 7, 60590 Frankfurt, Germany.
Clin Oral Investig. 2012 Jun;16(3):917-22. doi: 10.1007/s00784-011-0580-5. Epub 2011 Jun 17.
A prospective, randomized, controlled, split-mouth trial was performed to evaluate the cementation modes for metal-ceramic crowns. A total of 40 fully veneered metal-ceramic crowns were delivered in the posterior jaw segments of 20 patients using either a self-adhesive resin cement (RelyX Unicem Aplicap, 3M ESPE; n = 20) or a zinc oxide phosphate cement (Hoffmann's Cement, Hoffmann; n = 20). Thirteen parameters related to the abutment teeth and their periodontal status were evaluated. A visual analog scale was used to assess the sensitivity of the abutment teeth by patient-based outcomes. Data were statistically analyzed by a single-classification ANOVA (α = 0.05) and logistic regression analysis. The results presented were obtained after a mean observation period of 1.8 years. The dropout rate was 0%. None of the abutment teeth exhibited secondary caries at the restoration margins. No significant differences were demonstrated between the luting agents based on visual analog scale (p > 0.05), hypersensitivity (OR = 1.31), abutment mobility (p > 0.05), or probing depths (p > 0.05). Based on the sulcus fluid flow rates, a significantly greater mean difference was obtained with zinc oxide phosphate cement than with self-adhesive resin cement (9.2 units; p = 0.0006). Significant differences between the baseline examination and the follow-up examinations for sulcus bleeding index (p = 0.0013) and plaque index (p < 0.0001) were observed regardless of the luting agent used. The two cement types showed scarcely any differences between the parameters investigated. The outcomes of cementing fully veneered metal-ceramic crowns were equally good with self-adhesive resin cement as with the clinically proven zinc oxide phosphate cement.
一项前瞻性、随机、对照、分口研究评估了金属烤瓷冠的粘结方式。将 40 个全瓷面金属烤瓷冠分别用自粘结树脂水门汀(RelyX Unicem Aplicap,3M ESPE;n = 20)或氧化锌丁香油水门汀(Hoffmann's Cement,Hoffmann;n = 20)粘结于 20 名患者的下颌后牙段。评估了与基牙及其牙周状况相关的 13 个参数。通过患者为基础的结果使用视觉模拟评分评估基牙的敏感性。数据采用单分类方差分析(α = 0.05)和逻辑回归分析进行统计分析。结果在平均观察期 1.8 年后获得。失访率为 0%。修复体边缘无继发龋。两种粘结剂在视觉模拟评分(p > 0.05)、过敏反应(OR = 1.31)、基牙动度(p > 0.05)或探诊深度(p > 0.05)方面无显著差异。根据龈沟液流速,氧化锌丁香油水门汀的平均差值明显大于自粘结树脂水门汀(9.2 个单位;p = 0.0006)。无论使用何种粘结剂,龈沟出血指数(p = 0.0013)和菌斑指数(p < 0.0001)在基线检查和随访检查之间均有显著差异。两种粘结剂在研究的参数上差异不大。用自粘结树脂水门汀和临床证实的氧化锌丁香油水门汀粘结全瓷面金属烤瓷冠的效果相当好。