Biomaterials & Tissue Engineering Division, Department of Endodontics, Prosthodontics and Operative Dentistry, University of Maryland Dental School, Baltimore, MD 21201, USA.
Dent Mater. 2013 Apr;29(4):462-72. doi: 10.1016/j.dental.2013.01.011. Epub 2013 Feb 17.
Recent studies developed antibacterial bonding agents and composites containing a quaternary ammonium dimethacrylate (QADM) and nanoparticles of silver (NAg). The objectives of this study were to investigate: (1) the effect of antibacterial primers containing QADM and NAg on the inhibition of Streptococcus mutans impregnated into dentin blocks for the first time, and (2) the effect of QADM or NAg alone or in combination, and the effect of NAg mass fraction, on S. mutans viability in dentin.
Scotchbond Multi-Purpose (SBMP) bonding agent was used. QADM and NAg were incorporated into SBMP primer. Six primers were tested: SBMP primer control, control+10% QADM (mass%), control+0.05% NAg, control+10% QADM+0.05% NAg, control+0.1% NAg, and control+10% QADM+0.1% NAg. S. mutans were impregnated into dentin blocks, then a primer was applied. The viable colony-forming units (CFU) were then measured by harvesting the bacteria in dentin using a sonication method.
Control+10% QADM+0.1% NAg had bacteria inhibition zone 8-fold that of control (p<0.05). The sonication method successfully harvested bacteria from dentin blocks. Control+10% QADM+0.1% NAg inhibited S. mutans in dentin blocks, reducing the viable CFU in dentin by three orders of magnitude, compared to control dentin without primer. Using QADM+NAg was more effective than QADM alone. Higher NAg content increased the potency. Dentin shear bond strength was similar for all groups (p>0.1).
Antibacterial primer with QADM and NAg were shown to inhibit the S. mutans impregnated into dentin blocks for the first time. Bonding agent containing QADM and NAg is promising to eradicate bacteria in tooth cavity and inhibit caries. The QADM and NAg may have applicability to other adhesives, cements, sealants and composites.
最近的研究开发了含有季铵二甲基丙烯酸酯(QADM)和纳米银(NAg)的抗菌粘结剂和复合材料。本研究的目的是:(1)首次研究含有 QADM 和 NAg 的抗菌底漆对牙本质中变形链球菌的抑制作用;(2)单独使用 QADM 或 NAg,以及 QADM 和 NAg 联合使用时,以及 NAg 质量分数对牙本质中变形链球菌活力的影响。
使用 Scotchbond Multi-Purpose(SBMP)粘结剂。将 QADM 和 NAg 掺入 SBMP 底漆中。共测试了 6 种底漆:SBMP 底漆对照、对照+10% QADM(质量%)、对照+0.05% NAg、对照+10% QADM+0.05% NAg、对照+0.1% NAg 和对照+10% QADM+0.1% NAg。将变形链球菌注入牙本质块中,然后涂底漆。然后通过超声法从牙本质中收集细菌来测量活菌形成单位(CFU)。
对照+10% QADM+0.1% NAg 的抑菌圈是对照的 8 倍(p<0.05)。超声法成功地从牙本质块中收集到细菌。对照+10% QADM+0.1% NAg 抑制了牙本质块中的变形链球菌,与无底漆的牙本质相比,将牙本质中的活菌 CFU 减少了三个数量级。使用 QADM+NAg 比单独使用 QADM 更有效。较高的 NAg 含量增加了效力。各组的牙本质剪切粘结强度相似(p>0.1)。
首次证明含有 QADM 和 NAg 的抗菌底漆可抑制牙本质中变形链球菌的生长。含有 QADM 和 NAg 的粘结剂有望根除牙腔中的细菌并抑制龋齿。QADM 和 NAg 可能适用于其他粘结剂、水泥、密封剂和复合材料。