Abstract

OBJECTIVES

The aim of this study was to evaluate the linear and volumetric dimensional changes of six denture base resins processed by their corresponding injection-molding systems at 3 time intervals of water storage.

MATERIALS AND METHODS

Two heat-curing (SR Ivocap Hi Impact and Lucitone 199) and four auto-curing (IvoBase Hybrid, IvoBase Hi Impact, PalaXpress, and Futura Gen) acrylic resins were used with their specific injection-molding technique to fabricate 6 specimens of each material. Linear and volumetric dimensional changes were determined by means of a digital caliper and an electronic hydrostatic balance, respectively, after water storage of 1, 30, or 90 days. Means and standard deviations of linear and volumetric dimensional changes were calculated in percentage (%). Statistical analysis was done using Student's and Welch's t tests with Bonferroni-Holm correction for multiple comparisons (α=0.05).

RESULTS

Statistically significant differences in linear dimensional changes between resins were demonstrated at all three time intervals of water immersion (p≤0.05), with exception of the following comparisons which showed no significant difference: IvoBase Hi Impact/SR Ivocap Hi Impact and PalaXpress/Lucitone 199 after 1 day, Futura Gen/PalaXpress and PalaXpress/Lucitone 199 after 30 days, and IvoBase Hybrid/IvoBase Hi Impact after 90 days. Also, statistically significant differences in volumetric dimensional changes between resins were found at all three time intervals of water immersion (p≤0.05), with exception of the comparison between PalaXpress and Futura Gen.

SIGNIFICANCE

Denture base resins (IvoBase Hybrid and IvoBase Hi Impact) processed by the new injection-molding system (IvoBase), revealed superior dimensional precision.

摘要

目的

本研究旨在评估 6 种义齿基托树脂在浸水的 3 个时间间隔内,经相应注塑系统处理后的线性和体积尺寸变化。

材料与方法

使用 2 种热固性树脂(SR Ivocap Hi Impact 和 Lucitone 199)和 4 种自固化树脂(IvoBase Hybrid、IvoBase Hi Impact、PalaXpress 和 Futura Gen),分别采用特定的注塑技术制作每种材料的 6 个样本。线性和体积尺寸变化通过数字卡尺和电子静水天平分别在浸水 1、30 或 90 天后进行测量。线性和体积尺寸变化的平均值和标准差以百分比(%)表示。采用 Student's 和 Welch's t 检验以及多重比较的 Bonferroni-Holm 校正进行统计学分析(α=0.05)。

结果

在所有 3 个水浸泡时间间隔内,各树脂之间的线性尺寸变化均存在统计学显著差异(p≤0.05),但有 3 组比较无显著差异,分别为:第 1 天的 IvoBase Hi Impact/SR Ivocap Hi Impact 和 PalaXpress/Lucitone 199,第 30 天的 Futura Gen/PalaXpress 和 PalaXpress/Lucitone 199,以及第 90 天的 IvoBase Hybrid/IvoBase Hi Impact。此外,在所有 3 个水浸泡时间间隔内,各树脂之间的体积尺寸变化均存在统计学显著差异(p≤0.05),但 PalaXpress 和 Futura Gen 之间的比较除外。

意义

采用新型注塑系统(IvoBase)加工的义齿基托树脂(IvoBase Hybrid 和 IvoBase Hi Impact)具有更优异的尺寸精度。