Patil Seema S, M R Dhakshaini, Gujjari Anil Kumar
Professor and Head, Department of Prosthodontics, JSS Dental College and Hospital , Mysore, Karntaka, India .
J Clin Diagn Res. 2013 Sep;7(9):2056-9. doi: 10.7860/JCDR/2013/6086.3404. Epub 2013 Sep 10.
The discolouration of artificial teeth, which hampers aesthetics, is one of the negative effects of cigarette smoking. Therefore, the effect of cigarette smoke on the colour stability of commercially available acrylic resin teeth needs to be evaluated for clinical success and to ascertain as to which brand has superior properties.
Three commercially available acrylic teeth were evaluated, after division into Group A (Premadent), Group B (Astra), and Group C (Sanyo- Dent). Selected brands were subdivided as study group and control group. Each set of acrylic resin teeth were stored in artificial saliva at 37±1°C for 24 hours. After 24 hours of immersion, the colour measurement of each tooth (T0) was performed. Second colour measurements were done after 21 days (T21) of exposure to cigarette smoke for study group and after immersion in artificial saliva for control group. All data was statistically analyzed by using Repeated Measures ANOVA and Two-way ANOVA (p<0.05).
Group A showed least total colour change on exposure to cigarette smoke, followed by Group B and Group C had the highest total colour change. In control group, after immersion in artificial saliva, a slight increase in total colour change was observed for all groups, which was clinically acceptable.
Group A (crosslinked acrylic resin teeth) was more colour stable and more resistant to the discolouration which was caused by cigarette smoke, followed by Group B (crosslinked acrylic resin teeth). Group C (Non-crosslinked acrylic resin teeth) was least colour stable and most susceptible to discolouration which was caused by cigarette smoke.
假牙变色会影响美观,是吸烟的负面影响之一。因此,为了临床成功以及确定哪个品牌具有更优性能,需要评估香烟烟雾对市售丙烯酸树脂牙颜色稳定性的影响。
评估了三种市售丙烯酸牙,分为A组(Premadent)、B组(Astra)和C组(Sanyo-Dent)。选定的品牌再细分为研究组和对照组。每组丙烯酸树脂牙在37±1°C的人工唾液中储存24小时。浸泡24小时后,对每颗牙齿进行颜色测量(T0)。研究组在接触香烟烟雾21天后(T21)进行第二次颜色测量,对照组则在人工唾液中浸泡后进行测量。所有数据采用重复测量方差分析和双向方差分析进行统计学分析(p<0.05)。
A组在接触香烟烟雾后总颜色变化最小,其次是B组,C组总颜色变化最大。在对照组中,人工唾液浸泡后,所有组的总颜色变化均有轻微增加,在临床上是可接受的。
A组(交联丙烯酸树脂牙)颜色稳定性更高,对香烟烟雾引起的变色更具抵抗力,其次是B组(交联丙烯酸树脂牙)。C组(非交联丙烯酸树脂牙)颜色稳定性最差,最容易受到香烟烟雾引起的变色影响。