Javidi Maryam, Zarei Mina, Omidi Salma, Ghorbani Ahmad, Gharechahi Maryam, Shayani Rad Maryam
Dental Material Research Center, Department of Endodontics, Dental School, Mashhad University of Medical Sciences, Mashhad, Iran;
Department of Endodontics, Dental School, Mazandaran University of Medical Sciences, Sari, Iran ;
Iran Endod J. 2015 Fall;10(4):231-5. doi: 10.7508/iej.2015.04.004.
The aim of this study was to evaluate the cytotoxicity of a new nano zinc-oxide eugenol (NZOE) sealer in comparison with AH-26 and Pulpdent root canal sealers.
The L929 mouse fibroblast cells were cultivated and incubated for 24, 48 or 72 h with different dilutions (1/1, 1/2, 1/4, 1/8, 1/16 and 1/32) of culture media previously exposed to either of the test sealers naming NZOE, AH-26 or Pulpdent. At the end of incubation period, the effect of sealers on cell viability was evaluated using Mosmann's Tetrazolium Toxicity (MTT) colorimetric assay. The data was compared using the one-way analysis of variance (ANOVA) followed by the Tukey's post hoc test for multiple comparisons.
After 24, 48 or 72 h, both NZOE and Pulpdent sealers inhibited cell viability at 1/1, 1/2 and 1/8 dilutions. Within the 24 and 48 h, the AH-26 sealer reduced the cell viability at all dilutions except the 1/32 solution; however after 72 h even the 1/32 dilution was cytotoxic.
The biocompatibility of the nano zinc-oxide eugenol sealer was comparable to Pulpdent sealer and lower than AH-26.
本研究旨在评估一种新型纳米氧化锌丁香酚(NZOE)根管封闭剂与AH - 26和Pulpdent根管封闭剂相比的细胞毒性。
培养L929小鼠成纤维细胞,并用先前接触过NZOE、AH - 26或Pulpdent这三种测试封闭剂之一的不同稀释度(1/1、1/2、1/4、1/8、1/16和1/32)的培养基孵育24、48或72小时。在孵育期结束时,使用莫斯曼四唑盐毒性(MTT)比色法评估封闭剂对细胞活力的影响。数据采用单因素方差分析(ANOVA)进行比较,随后进行Tukey事后检验以进行多重比较。
在24、48或72小时后,NZOE和Pulpdent封闭剂在1/1、1/2和1/8稀释度下均抑制细胞活力。在24小时和48小时内,AH - 26封闭剂在除1/32溶液外的所有稀释度下均降低细胞活力;然而在72小时后,即使是1/32稀释度也具有细胞毒性。
纳米氧化锌丁香酚封闭剂的生物相容性与Pulpdent封闭剂相当,低于AH - 26。