Suppr超能文献

磷酸预蚀刻时间对通用粘合剂粘结耐久性及牙釉质表面自由能特性的影响

Influence of duration of phosphoric acid pre-etching on bond durability of universal adhesives and surface free-energy characteristics of enamel.

作者信息

Tsujimoto Akimasa, Barkmeier Wayne W, Takamizawa Toshiki, Watanabe Hidehiko, Johnson William W, Latta Mark A, Miyazaki Masashi

机构信息

Department of Operative Dentistry, Nihon University School of Dentistry, Tokyo, Japan.

Department of General Dentistry, Creighton University School of Dentistry, Omaha, NE, USA.

出版信息

Eur J Oral Sci. 2016 Aug;124(4):377-86. doi: 10.1111/eos.12284. Epub 2016 Jun 18.

Abstract

The purpose of this study was to evaluate the influence of duration of phosphoric acid pre-etching on the bond durability of universal adhesives and the surface free-energy characteristics of enamel. Three universal adhesives and extracted human molars were used. Two no-pre-etching groups were prepared: ground enamel; and enamel after ultrasonic cleaning with distilled water for 30 s to remove the smear layer. Four pre-etching groups were prepared: enamel pre-etched with phosphoric acid for 3, 5, 10, and 15 s. Shear bond strength (SBS) values of universal adhesive after no thermal cycling and after 30,000 or 60,000 thermal cycles, and surface free-energy values of enamel surfaces, calculated from contact angle measurements, were determined. The specimens that had been pre-etched showed significantly higher SBS and surface free-energy values than the specimens that had not been pre-etched, regardless of the aging condition and adhesive type. The SBS and surface free-energy values did not increase for pre-etching times of longer than 3 s. There were no significant differences in SBS values and surface free-energy characteristics between the specimens with and without a smear layer. The results of this study suggest that phosphoric acid pre-etching of enamel improves the bond durability of universal adhesives and the surface free-energy characteristics of enamel, but these bonding properties do not increase for phosphoric acid pre-etching times of longer than 3 s.

摘要

本研究的目的是评估磷酸预蚀刻时间对通用粘合剂粘结耐久性以及牙釉质表面自由能特性的影响。使用了三种通用粘合剂和拔除的人类磨牙。制备了两个未预蚀刻组:磨除牙釉质;以及用蒸馏水超声清洗30秒以去除玷污层后的牙釉质。制备了四个预蚀刻组:用磷酸预蚀刻3、5、10和15秒的牙釉质。测定了未进行热循环以及进行30000次或60000次热循环后通用粘合剂的剪切粘结强度(SBS)值,以及通过接触角测量计算得到的牙釉质表面自由能值。无论老化条件和粘合剂类型如何,预蚀刻的标本显示出比未预蚀刻的标本显著更高的SBS和表面自由能值。预蚀刻时间超过3秒时,SBS和表面自由能值并未增加。有玷污层和无玷污层的标本之间,SBS值和表面自由能特性没有显著差异。本研究结果表明,牙釉质的磷酸预蚀刻可提高通用粘合剂的粘结耐久性和牙釉质的表面自由能特性,但磷酸预蚀刻时间超过3秒时,这些粘结性能不会增加。