Nebergall A K, Greene M E, Laursen M B, Nielsen P T, Malchau H, Troelsen A
Massachusetts General Hospital, 55 Fruit Street, Boston, MA, 02114, USA.
Aalborg University Hospital, Hobrovej 18-22, Aalborg, Denmark.
Bone Joint J. 2017 May;99-B(5):577-584. doi: 10.1302/0301-620X.99B5.37521.
The objective of this five-year prospective, blinded, randomised controlled trial (RCT) was to compare femoral head penetration into a vitamin E diffused highly cross-linked polyethylene (HXLPE) liner with penetration into a medium cross-linked polyethylene control liner using radiostereometric analysis.
Patients scheduled for total hip arthroplasty (THA) were randomised to receive either the study E1 (32 patients) or the control ArComXL polyethylene (35 patients). The median age (range) of the overall cohort was 66 years (40 to 76).
The five-year median (interquartile range) proximal femoral head penetration into the E1 was -0.05 mm (-0.13 to -0.02) and 0.07 mm (-0.03 to 0.16) for ArComXL. At three and five years, the penetration was significantly greater in the ArComXL group compared with the E1 group (p = 0.029 and p = 0.019, respectively). All patient-reported outcomes (PROs) improved significantly from the pre-operative interval compared with those at one year, and remained favourable at five years. There were no differences between the two groups at any interval.
The five-year results showed that E1 polyethylene does not wear more than the control, ArComXL. This is the longest-term RCT comparing the wear performance and clinical outcome of vitamin E diffused HXLPE with a previous generation of medium cross-linked polyethylene. Cite this article: 2017;99-B:577-84.
这项为期五年的前瞻性、双盲、随机对照试验(RCT)的目的是,使用放射立体分析比较股骨头在维生素E扩散的高交联聚乙烯(HXLPE)内衬中的穿透情况与在中交联聚乙烯对照内衬中的穿透情况。
计划接受全髋关节置换术(THA)的患者被随机分为两组,分别接受研究用E1内衬(32例患者)或对照用ArComXL聚乙烯内衬(35例患者)。整个队列的中位年龄(范围)为66岁(40至76岁)。
五年时,股骨头近端在E1内衬中的中位(四分位间距)穿透为-0.05毫米(-0.13至-0.02),在ArComXL内衬中为0.07毫米(-0.03至0.16)。在三年和五年时,ArComXL组的穿透明显大于E1组(分别为p = 0.029和p = 0.019)。与术前相比,所有患者报告结局(PROs)在术后一年均有显著改善,且在五年时仍保持良好。两组在任何时间点均无差异。
五年结果表明,E1聚乙烯的磨损不超过对照组ArComXL。这是比较维生素E扩散的HXLPE与上一代中交联聚乙烯磨损性能和临床结局的最长时间的RCT。引用本文:2017;99-B:577-84。