Esmaeili Behnaz, Abolghasemzadeh Faezeh, Gholampor Atefeh, Daryakenari Ghazaleh
Gen Dent. 2018 Jan-Feb;66(1):40-44.
Bleaching is a conservative treatment for discolored teeth, but the effect of this treatment on newer, silorane-based composite resins is unclear. This study evaluated the effect of at-home bleaching on the microhardness of methacrylate- and silorane-based composites. Forty blocks each of a methacrylate-based composite and a silorane-based composite were prepared. The 80 specimens were tested in 8 groups (n = 10): 2 composites, each exposed to 3 different carbamide peroxide concentrations (10%, 16%, or 22%) as well as distilled water (control). The surface of the test specimens was covered daily with the bleaching gel at room temperature for the time period recommended by the manufacturer for each carbamide peroxide concentration. A Vickers hardness testing machine was used with a 100-g load for 20 seconds to register specimen microhardness prior to and after 2 weeks of bleaching. The load was applied at 3 points, and the mean microhardness was calculated. Repeated-measures analysis of variance, paired t test, and Tukey test were used to analyze the data. All bleaching concentrations significantly decreased the microhardness of the methacrylate-based composite resin groups, while microhardness was significantly increased in the silorane-based composite resin groups. There was no evident difference in effects among the different gel concentrations (P > 0.05).
牙齿美白是一种针对变色牙齿的保守治疗方法,但这种治疗方法对新型的、基于硅氧烷的复合树脂的效果尚不清楚。本研究评估了家庭牙齿美白对甲基丙烯酸酯基和硅氧烷基复合树脂显微硬度的影响。制备了甲基丙烯酸酯基复合树脂和硅氧烷基复合树脂各40个试件。80个样本分为8组进行测试(每组n = 10):两种复合树脂,每种分别暴露于3种不同浓度的过氧化脲(10%、16%或22%)以及蒸馏水(对照组)。在室温下,按照每种过氧化脲浓度制造商推荐的时间,每天用美白凝胶覆盖测试样本的表面。使用维氏硬度测试机,在100克载荷下加载20秒,以记录美白2周前后样本的显微硬度。在3个点施加载荷,并计算平均显微硬度。采用重复测量方差分析、配对t检验和Tukey检验对数据进行分析。所有美白浓度均显著降低了甲基丙烯酸酯基复合树脂组的显微硬度,而硅氧烷基复合树脂组的显微硬度显著增加。不同凝胶浓度之间的效果没有明显差异(P > 0.05)。