Suppr超能文献

与龋损牙本质的粘结。

Bonding to caries affected dentine.

机构信息

Department of Endodontics, School of Dentistry, Tehran University of Medical Sciences, Tehran, Iran.

Department of Endodontics, School of Dentistry, Tehran University of Medical Sciences, Tehran, Iran,; Endodontology Research Group, School of Dentistry, Cardiff University, Cardiff, Wales, UK.

出版信息

Dent Mater. 2018 Sep;34(9):e236-e245. doi: 10.1016/j.dental.2018.05.017. Epub 2018 Jun 8.

Abstract

OBJECTIVES

Dentine replacement materials are often placed over caries affected dentine (CAD). The aim of this study was to compare the bonding characteristics and interactions of selected hydraulic calcium silicate-based dentine replacement materials to CAD and sound dentine.

METHODS

Three hydraulic calcium silicate-based dentine replacement materials were assessed: Retro MTA, Biodentine and Theracal LC. Material characterization was done by scanning electron microscopy and X-ray diffraction analyses. Blocks of sound and CAD were prepared and standardized by Vickers microhardness testing. Half of the affected and sound dentine blocks were pretreated with 5.25% NaOCl prior to material placement. The materials were stored either for 1 week or 24 weeks in 37°C in fully saturated conditions. Shear bond strength was assessed at both time periods. Radiopacity of the interfacial dentine was also evaluated to assess the remineralization potential of the dentine replacement materials.

RESULTS

The reaction of Theracal was slower than that of the water-based materials. The bond strengths of different materials did not differ after 1 week (P>0.05). The bond strength of Biodentine and Retro MTA increased over time but no change was observed for Theracal. NaOCl pre-treatment deteriorated the bond strength to sound dentine but improvement was observed in affected dentine. Radiopacity changes were observed after 24 weeks.

SIGNIFICANCE

Biodentine and Retro MTA showed better bonding to CAD. Pretreatment with NaOCl improved the bond strength of dentine replacement materials to CAD.

摘要

目的

牙本质替代材料通常放置在受龋影响的牙本质(CAD)上。本研究的目的是比较选定的水硬硅酸钙基牙本质替代材料与 CAD 和正常牙本质的粘结特性和相互作用。

方法

评估了三种水硬硅酸钙基牙本质替代材料:Retro MTA、Biodentine 和 Theracal LC。通过扫描电子显微镜和 X 射线衍射分析进行材料特性分析。制备和标准化正常和 CAD 牙本质块,采用维氏显微硬度测试。将一半受影响和正常牙本质块用 5.25% NaOCl 预处理,然后放置材料。将材料在 37°C 下完全饱和条件下储存 1 周或 24 周。在两个时间段评估剪切粘结强度。还评估了界面牙本质的射线不透性,以评估牙本质替代材料的再矿化潜力。

结果

Theracal 的反应速度比水基材料慢。1 周后,不同材料的粘结强度没有差异(P>0.05)。Biodentine 和 Retro MTA 的粘结强度随时间增加而增加,但 Theracal 没有变化。NaOCl 预处理会降低正常牙本质的粘结强度,但在受影响的牙本质中观察到改善。24 周后观察到射线不透性变化。

意义

Biodentine 和 Retro MTA 对 CAD 的粘结性更好。NaOCl 预处理可提高牙本质替代材料对 CAD 的粘结强度。