不同自粘结树脂水门汀的细胞毒性作用:细胞活力与凋亡诱导

Cytotoxic effects of different self-adhesive resin cements: Cell viability and induction of apoptosis.

作者信息

Şişmanoğlu Soner, Demirci Mustafa, Schweikl Helmut, Ozen-Eroglu Gunes, Cetin-Aktas Esin, Kuruca Serap, Tuncer Safa, Tekce Neslihan

机构信息

Department of Restorative Dentistry, Faculty of Dentistry, Altınbaş University, Istanbul, Turkey.

Department of Restorative Dentistry, Faculty of Dentistry, Istanbul University, Istanbul, Turkey.

出版信息

J Adv Prosthodont. 2020 Apr;12(2):89-99. doi: 10.4047/jap.2020.12.2.89. Epub 2020 Apr 22.

Abstract

PURPOSE

The effects of four different self-adhesive resin cement materials on cell viability and apoptosis after direct and indirect exposure were evaluated using different cell culture techniques.

MATERIALS AND METHODS

Self-adhesive cements were applied to NIH/3T3 mouse fibroblasts by the extract test method, cell culture inserts, and dentin barrier test method. After exposure periods of 24 h and 72 h, the cytotoxicity of these self-adhesive materials was evaluated using the MTT assay (viability) and the Annexin-V-FITC/PI staining (apoptosis).

RESULTS

The lowest cell viability was found in cells exposed to BeautiCem SA for 24 h in the extract test method. Cell viability was reduced to 70.6% compared to negative controls. After the 72 h exposure period, viability rate of cell cultures exposed to BeautiCem SA decreased more than 2- fold (29.5%) while cells exposed to RelyX U200 showed the highest viability rate of 71.4%. In the dentin barrier test method, BeautiCem SA induced the highest number of cells in apoptosis after a 24 h exposure (4.1%). Panavia SA Cement Plus was the material that caused the lowest number of cells in apoptosis (1.5%).

CONCLUSION

The used self-adhesive cements have showed different cytotoxic effects based on the evaluation method. As exposure time increased, the materials showed more cytotoxic and apoptotic effects. BeautiCem SA caused significantly more severe cytotoxic and apoptotic effects than other cements tested. Moreover, cements other than BeautiCem SA have caused necrotic cell death rather than apoptotic cell death.

摘要

目的

采用不同细胞培养技术,评估四种不同的自粘树脂水门汀材料在直接和间接接触后对细胞活力和凋亡的影响。

材料与方法

通过提取物测试法、细胞培养插入物法和牙本质屏障测试法,将自粘水门汀应用于NIH/3T3小鼠成纤维细胞。在暴露24小时和72小时后,使用MTT法(活力)和Annexin-V-FITC/PI染色法(凋亡)评估这些自粘材料的细胞毒性。

结果

在提取物测试法中,暴露于BeautiCem SA 24小时的细胞活力最低。与阴性对照相比,细胞活力降至70.6%。暴露72小时后,暴露于BeautiCem SA的细胞培养物活力率下降超过2倍(29.5%),而暴露于RelyX U200的细胞活力率最高,为71.4%。在牙本质屏障测试法中,暴露24小时后,BeautiCem SA诱导的凋亡细胞数量最多(4.1%)。Panavia SA Cement Plus是导致凋亡细胞数量最少的材料(1.5%)。

结论

根据评估方法,所用的自粘水门汀表现出不同的细胞毒性作用。随着暴露时间的增加,材料表现出更强的细胞毒性和凋亡作用。与其他测试的水门汀相比,BeautiCem SA引起的细胞毒性和凋亡作用明显更严重。此外,除BeautiCem SA外的水门汀导致的是坏死性细胞死亡而非凋亡性细胞死亡。

https://cdn.ncbi.nlm.nih.gov/pmc/blobs/dd0e/7183849/4484159ded2f/jap-12-89-g001.jpg