Suppr超能文献

青少年中微混合复合材料和纳米复合材料暴露于常见软饮料后颜色稳定性的分光光度法比较:一项体外研究。

Spectrophotometric comparison of color stability of microhybrid and nanocomposites following exposure to common soft drinks among adolescents: an in vitro study.

作者信息

Al-Haj Ali S N, Alsulaim H N, Albarrak M I, Farah R I

机构信息

Department of Orthodontic and Pediatric Dentistry, College of Dentistry, Qassim University, PO Box: 6700, Qassim, 51452, Saudi Arabia.

College of Dentistry, Qassim University, Qassim, Saudi Arabia.

出版信息

Eur Arch Paediatr Dent. 2021 Aug;22(4):675-683. doi: 10.1007/s40368-021-00605-6. Epub 2021 Feb 10.

Abstract

PURPOSE

To compare the color stability of a microhybrid and two nanocomposites after exposure to common soft drinks among adolescents.

METHODS

Ninety discs were prepared from a microhybrid (Filtek Z250) and two nanocomposites (Filtek Z350 and Tetric N-Ceram) (n = 30 each). Six discs from each material were then immersed in one of five drinks (iced tea, sports drink, orange juice, cola, and distilled water) for 15 days. Color measurement was performed at baseline and after 15 days using a spectrophotometer according to the CIE Lab* system, and the change in color values as well as total color change (ΔE) was calculated and compared. ANOVA and Tukey's HSD test were used to analyze the data (p < 0.05).

RESULTS

Significant change in color values and total color (ΔE > 3.3) was observed in the composite materials after immersion in the soft drinks compared to immersion in distilled water (ΔE < 3.3). The highest mean values were those of Filtek Z350, being significantly different from the rest of the materials. Independent of the composite material, iced tea resulted in the highest mean values, being significantly different from the rest of the drinks (p < 0.05).

CONCLUSION

All soft drinks resulted in clinically unacceptable discoloration of the composite materials with maximum discoloration being that following immersion of composite materials, particularly Filtek Z350, in iced tea. Consequently, in dental practice, adolescents should be asked about their consumption of soft drinks, particularly iced tea, and made aware of their potential to discolor composite restorations if they are to receive them.

摘要

目的

比较青少年中一种微混合树脂和两种纳米复合树脂在接触常见软饮料后的颜色稳定性。

方法

用一种微混合树脂(Filtek Z250)和两种纳米复合树脂(Filtek Z350和Tetric N-Ceram)制备90个圆盘(每种n = 30)。然后将每种材料的6个圆盘浸入五种饮料(冰茶、运动饮料、橙汁、可乐和蒸馏水)之一中15天。在基线和15天后,使用分光光度计根据CIE Lab*系统进行颜色测量,并计算和比较颜色值的变化以及总颜色变化(ΔE)。采用方差分析和Tukey's HSD检验分析数据(p < 0.05)。

结果

与浸入蒸馏水中(ΔE < 3.3)相比,复合材料浸入软饮料后颜色值和总颜色(ΔE > 3.3)有显著变化。Filtek Z350的平均值最高,与其他材料有显著差异。与复合材料无关,冰茶导致的平均值最高,与其他饮料有显著差异(p < 0.05)。

结论

所有软饮料都会导致复合材料出现临床上不可接受的变色,最大变色情况是复合材料,尤其是Filtek Z350浸入冰茶后。因此,在牙科实践中,应询问青少年软饮料的饮用情况,特别是冰茶,并告知他们如果要接受复合树脂修复,饮用软饮料可能会导致修复体变色。