Suppr超能文献

非热大气等离子体对粘合剂/牙本质界面微拉伸粘结强度的影响:一项系统评价

Effect of Non-Thermal Atmospheric Plasma on Micro-Tensile Bond Strength at Adhesive/Dentin Interface: A Systematic Review.

作者信息

Awad Mohamed M, Alhalabi Feras, Alshehri Abdullah, Aljeaidi Zaid, Alrahlah Ali, Özcan Mutlu, Hamama Hamdi Hosni

机构信息

Department of Conservative Dental Sciences, College of Dentistry, Prince Sattam Bin Abdulaziz University, Al-Kharj 11942, Saudi Arabia.

Department of Restorative Dental Science, College of Dentistry, King Saud University, Riyadh 11545, Saudi Arabia.

出版信息

Materials (Basel). 2021 Feb 22;14(4):1026. doi: 10.3390/ma14041026.

Abstract

OBJECTIVE

The objective of this review was to evaluate the effect of non-thermal atmospheric plasma (NTAP) on adhesives resin-dentin micro-tensile bond strength (μTBS) in previously published studies.

METHODS

Electronic search was conducted using the Medline, Cochrane library, and Scopus databases. The included studies were laboratory studies that investigated the effect of NTAP on adhesives μTBS to coronal dentin. Studies that evaluated the effect of NTAP on bond strength to indirect substrates, enamel or root dentin, were excluded. The methodological quality of included studies was assessed.

RESULTS

Thirteen studies were included in this systematic review. All the included studies were considered to have a medium risk of bias. NTAP significantly improved μTBS at 24 h or after short-term aging in five studies (38.5%) and both immediate and after long-term aging in 5 studies (38.5%). In two studies (15.4%), NTAP resulted in a short-term material-dependent effect that was not stable after long-term aging. Interestingly, in one study (7.7%), NTAP had a positive effect only in the etch-and-rinse (ER) mode after long-term aging.

CONCLUSION

Within the limitations of this systematic review, NTAP application could enhance resin-dentin μTBS of ER adhesives or universal adhesives (UAs) applied in the ER mode. In the ER mode, the rewetting step after NTAP seems to be unnecessary. Because of the limited information currently available in the literature, further studies are required to evaluate the effect of the NTAP application on self-etch (SE) adhesives or UAs applied in the SE mode.

摘要

目的

本综述的目的是评估非热大气等离子体(NTAP)对先前已发表研究中粘合剂与牙本质的微拉伸粘结强度(μTBS)的影响。

方法

使用Medline、Cochrane图书馆和Scopus数据库进行电子检索。纳入的研究为实验室研究,其调查了NTAP对粘合剂与冠部牙本质μTBS的影响。评估NTAP对间接底物、釉质或根部牙本质粘结强度影响的研究被排除。对纳入研究的方法学质量进行了评估。

结果

本系统综述纳入了13项研究。所有纳入研究均被认为存在中度偏倚风险。在5项研究(38.5%)中,NTAP在24小时或短期老化后显著提高了μTBS,在5项研究(38.5%)中,NTAP在即刻和长期老化后均显著提高了μTBS。在2项研究(15.4%)中,NTAP产生了短期的材料依赖性效应,长期老化后不稳定。有趣的是,在1项研究(7.7%)中,NTAP仅在长期老化后的酸蚀冲洗(ER)模式下具有积极作用。

结论

在本系统综述的局限性内,应用NTAP可提高ER粘合剂或在ER模式下应用的通用粘合剂(UAs)的树脂-牙本质μTBS。在ER模式下,NTAP后的再湿润步骤似乎不必要。由于目前文献中的信息有限,需要进一步研究来评估应用NTAP对自酸蚀(SE)粘合剂或在SE模式下应用的UAs的影响。

https://cdn.ncbi.nlm.nih.gov/pmc/blobs/c5ce/7926439/6da3b38a48aa/materials-14-01026-g001.jpg

文献AI研究员

20分钟写一篇综述,助力文献阅读效率提升50倍。

立即体验

用中文搜PubMed

大模型驱动的PubMed中文搜索引擎

马上搜索

文档翻译

学术文献翻译模型,支持多种主流文档格式。

立即体验