Kobetičová Klára, Böhm Martin, Jerman Miloš, Dušek Jaroslav, Černý Robert
Department of Materials Engineering and Chemistry, Faculty of Civil Engineering, Czech Technical University in Prague, Thákurova 7, 166 29 Prague, Czech Republic.
Polymers (Basel). 2022 May 29;14(11):2209. doi: 10.3390/polym14112209.
Bone glue with sodium lignosulfonate is a protein-based adhesive. Their combination leads to strong binding necessary for the achievement of adhesive properties. However, biodegradation and ecotoxicity of materials composed of bone glue and sodium lignosulfonate has never been studied before. In this paper, the biodegradation potential of the mixture of bone glue, lignosulfonate and rape straw modified by water or NaOH on an agar test with aerial molds and in acute aquatic tests with mustard, yeasts, algae and crustaceans was analyzed. Epoxy resin as an ecologically unfriendly binder was used as a negative control and pure rape straw as a background. The results indicated that all samples were covered by molds, but the samples containing straw treated by NaOH showed lower biodegradability. The ecotoxicological effects varied among the applied model organisms. was not able to survive and could not prolong roots in the eluates of all samples (100% inhibition). Freshwater algae () were not significantly affected by the samples (max. 12% inhibition, max. 16% stimulation). The biomass of yeasts () was strongly stimulated in the presence of eluates in a comparison to control (max. 38% stimulation).
含有木质素磺酸钠的骨胶是一种基于蛋白质的粘合剂。它们的结合产生了实现粘合性能所需的强力粘合。然而,由骨胶和木质素磺酸钠组成的材料的生物降解性和生态毒性此前从未被研究过。本文分析了骨胶、木质素磺酸盐和用水或氢氧化钠改性的油菜秸秆混合物在琼脂培养基上对气生霉菌的生物降解潜力,以及在芥菜、酵母、藻类和甲壳类动物的急性水生试验中的生物降解潜力。环氧树脂作为一种生态不友好型粘合剂用作阴性对照,纯油菜秸秆用作背景。结果表明,所有样品都被霉菌覆盖,但含有经氢氧化钠处理秸秆的样品显示出较低的生物降解性。在应用的模式生物中,生态毒理学效应各不相同。在所有样品的洗脱液中均无法存活,且无法使根延长(100%抑制)。淡水藻类()受样品影响不显著(最大抑制率12%,最大刺激率16%)。与对照相比,在有洗脱液存在的情况下,酵母()的生物量受到强烈刺激(最大刺激率38%)。