Suppr超能文献

光动力疗法和氢氧化钙药物对玻璃纤维桩与根管内牙本质粘结界面性能影响的体外研究

In vitro study on how photodynamic therapy and calcium hydroxide medication influence adhesive interface properties of glass-fiber posts to intraradicular dentin.

作者信息

Strazzi-Sahyon Henrico Badaoui, Banci Henrique Augusto, Melo Fernanda Santos de, Soares Lucas Silva, Spin-Neto Rubens, Duarte Marco Antonio Hungaro, Cintra Luciano Tavares Angelo, Dos Santos Paulo Henrique, Sivieri-Araujo Gustavo

机构信息

Department of Dental Materials and Prosthodontics, Araçatuba School of Dentistry, São Paulo State University, UNESP, Araçatuba, SP, Brazil; Department of Prosthodontics and Periodontology, Bauru School of Dentistry, University of Sao Paulo, USP, Bauru, SP, Brazil.

Department of Preventive and Restorative Dentistry, Discipline of Endodontics, Araçatuba School of Dentistry, São Paulo State University, UNESP, Araçatuba, SP, Brazil.

出版信息

J Mech Behav Biomed Mater. 2023 May;141:105757. doi: 10.1016/j.jmbbm.2023.105757. Epub 2023 Mar 5.

Abstract

PURPOSE

This in vitro study evaluated the influence of antimicrobial photodynamic therapy (aPDT), using methylene blue (MB) as photosensitizer (PS) and calcium hydroxide (CH) as intracanal medication on adhesive bond strength, sealing, and integrity of the luting interface of glass-fiber posts to different thirds of endodontically treated root canal dentin.

MATERIAL AND METHODS

102 incisors were sorted into 6 groups: a negative control irrigated with deionized water; a positive control irrigated with deionized water and filled with CH; CH + MB 50 mg/L without laser radiation; CH + MB 100 mg/L without laser radiation; CH + MB 50 mg/L radiated by red laser; and CH + MB 100 mg/L radiated by red laser. Push-out bond strength (n = 8), adhesive interface sealing (n = 3), and volume and quantification of voids (n = 6) were assessed using a universal testing machine, confocal laser scanning microscope, and computerized microtomography, respectively. Scanning electron micrographs were obtained from representative samples to qualify the fracture patterns. Push-out bond strength and adhesive interface integrity data were subjected to 2-way ANOVA for repeated measures followed by Tukey's test (α = 0.05). Adhesive interface sealing was evaluated by the inter-examiner Kappa test and submitted to Kruskal-Wallis and Dunns tests (α = 0.05).

RESULTS

Assessing the apical region, the positive control and MB + Ca(OH) groups showed lower adhesive bond strength compared to the MB + Ca(OH) group (P < 0.05). The cervical third showed higher bond strength than the apical third for the positive control, MB + Ca(OH) MB + Ca(OH) and MB + Ca(OH) groups (P < 0.05). A prevalence of mixed failure was observed in all experimental groups. There were no statistically significant differences in adhesive interface sealing for any of the parameters assessed (P > 0.05). MB + Ca(OH) and MB + Ca(OH) groups promoted a higher volume and quantification of voids compared to the negative control group evaluating the cervical third (P < 0.05). In general, there were no differences in the quantification of voids comparing the intraradicular thirds (P > 0.05), differently to the volume of voids in which, in general, the cervical third promoted higher values compared to the middle and apical thirds (P < 0.05).

CONCLUSION

aPDT with methylene blue PS at 50 mg/L associated with calcium hydroxide as intracanal medication demonstrated satisfactory bond strength, sealing, and integrity of the adhesive interface at any intraradicular depth.

摘要

目的

本体外研究评估了以亚甲蓝(MB)作为光敏剂(PS)、氢氧化钙(CH)作为根管内用药的抗菌光动力疗法(aPDT)对玻璃纤维桩与根管治疗后根管牙本质不同三分之一处粘接界面的粘接强度、密封性和完整性的影响。

材料与方法

将102颗切牙分为6组:用去离子水冲洗的阴性对照组;用去离子水冲洗并充填CH的阳性对照组;50mg/L CH + MB且无激光照射组;100mg/L CH + MB且无激光照射组;50mg/L CH + MB经红色激光照射组;100mg/L CH + MB经红色激光照射组。分别使用万能试验机、共聚焦激光扫描显微镜和计算机断层扫描评估推出粘接强度(n = 8)、粘接界面密封性(n = 3)以及空隙的体积和定量分析(n = 6)。从代表性样本获取扫描电子显微镜图像以鉴定断裂模式。推出粘接强度和粘接界面完整性数据进行重复测量的双向方差分析,随后进行Tukey检验(α = 0.05)。粘接界面密封性通过检查者间Kappa检验进行评估,并进行Kruskal-Wallis和Dunns检验(α = 0.05)。

结果

在评估根尖区域时,阳性对照组和MB + Ca(OH)组的粘接强度低于MB + Ca(OH)组(P < 0.05)。对于阳性对照组、MB + Ca(OH) MB + Ca(OH)和MB + Ca(OH)组,颈部三分之一处的粘接强度高于根尖三分之一处(P < 0.05)。在所有实验组中均观察到混合性破坏占优势。在所评估的任何参数中,粘接界面密封性均无统计学显著差异(P > 0.05)。与评估颈部三分之一处的阴性对照组相比,MB + Ca(OH)和MB + Ca(OH)组促进了更高的空隙体积和定量分析(P < 0.05)。总体而言,比较根管内不同三分之一处的空隙定量分析无差异(P > 0.05),与空隙体积不同,总体而言,颈部三分之一处的空隙体积值高于中部和根尖三分之一处(P < 0.05)。

结论

50mg/L亚甲蓝PS的aPDT与氢氧化钙作为根管内用药联合使用,在根管内任何深度均表现出令人满意的粘接强度、密封性和粘接界面完整性。