: Magnetic resonance imaging (MRI) is widely used in diagnostics, but its effects on orthodontic materials remain a concern. This study aimed to evaluate the impact of MRI exposure at 1.5 T and 3 T on the shear bond strength (SBS) and adhesive remnant index (ARI) of different orthodontic bracket types (metal, self-ligating, and ceramic). : A total of 90 extracted human premolars were divided into three groups (control, 1.5 T, and 3 T MRI exposure). The three bracket types were bonded using Transbond XT adhesive and subjected to standardized polymerization. MRI scans were conducted using 1.5 T and 3 T machines with clinically relevant sequences. SBS was measured using a universal testing machine, and the ARI was assessed under a stereomicroscope. Statistical analysis was performed using Kruskal-Wallis and chi-square tests. : MRI exposure influenced SBS and the ARI differently across bracket types. Firstly, 3 T MRI exposure significantly reduced SBS in self-ligating ( = 0.017) and ceramic brackets ( = 0.014) compared to the control, whereas metal brackets showed no significant changes. ARI scores varied across MRI conditions, with metal and self-ligating brackets showing increased adhesive retention at higher field strengths. No significant differences were observed in ARI scores for ceramic brackets across MRI conditions. : The clinical importance of understanding these results is that both patients and clinicians must be aware of inevitable changes that occur in SBS during MRI, since exposure to high-field MRI, particularly 3 T, may alter bond strength and adhesive failure characteristics.
磁共振成像(MRI)在诊断中被广泛应用,但其对正畸材料的影响仍令人担忧。本研究旨在评估1.5T和3T的MRI暴露对不同类型正畸托槽(金属、自锁和陶瓷)的剪切粘结强度(SBS)和粘结剂残留指数(ARI)的影响。
共90颗拔除的人类前磨牙被分为三组(对照组、1.5T MRI暴露组和3T MRI暴露组)。使用Transbond XT粘结剂粘结三种托槽类型,并进行标准化聚合。使用1.5T和3T设备及临床相关序列进行MRI扫描。使用万能试验机测量SBS,并在体视显微镜下评估ARI。使用Kruskal-Wallis检验和卡方检验进行统计分析。
MRI暴露对不同托槽类型的SBS和ARI影响不同。首先,与对照组相比,3T MRI暴露显著降低了自锁托槽(P = 0.017)和陶瓷托槽(P = 0.014)的SBS,而金属托槽无显著变化。ARI评分在不同MRI条件下有所不同,金属和自锁托槽在更高场强下显示出粘结剂保留增加。陶瓷托槽在不同MRI条件下的ARI评分无显著差异。
理解这些结果的临床意义在于,患者和临床医生都必须意识到MRI过程中SBS会不可避免地发生变化,因为暴露于高场MRI,尤其是3T,可能会改变粘结强度和粘结失败特征。