全瓷冠的断裂强度

Fracture strength of all-ceramic crowns.

作者信息

Yoshinari M, Dérand T

机构信息

Department of Dental Materials Science, Tokyo Dental College, Chiba, Japan.

出版信息

Int J Prosthodont. 1994 Jul-Aug;7(4):329-38.

PMID:7993544
Abstract

The fracture strengths of four types of all-ceramic premolar crowns (conventional Vita-Dur, In-Ceram, Dicor, and IPS-Empress) were compared after a preload cycling in aqueous atmosphere. Preload cycling significantly decreased the strength of Vita-Dur crowns. Fracture strength of Vita-Dur crowns was improved when they were luted with either polyalkenoate or adhesive resin cement. The average (standard deviation) of load to fracture of ceramic crowns luted using zinc phosphate cement and after applied preload cycling in distilled water were: Vita Dur, 770 (237) N; Vita In-Ceram, 1060 (341) N; Dicor, 840 (226) N; and IPS-Empress: 891 (185) N. The In-Ceram crowns fractured in two modes: complete fractures at 1276 (207) N; and fractures with the core remaining intact at 808 (292) N.

摘要

在水气氛中进行预加载循环后,比较了四种类型的全瓷前磨牙冠(传统的维他 - 杜尔、In-Ceram、Dicor和IPS-Empress)的断裂强度。预加载循环显著降低了维他 - 杜尔冠的强度。当用聚羧酸酯或粘结树脂粘结剂粘结维他 - 杜尔冠时,其断裂强度得到提高。使用磷酸锌粘结剂粘结并在蒸馏水中进行预加载循环后,陶瓷冠的平均(标准差)断裂载荷为:维他 - 杜尔,770(237)N;维他In-Ceram,1060(341)N;Dicor,840(226)N;以及IPS-Empress:891(185)N。In-Ceram冠有两种断裂模式:在1276(207)N时完全断裂;在808(292)N时核心保持完整的断裂。

文献检索

告别复杂PubMed语法,用中文像聊天一样搜索,搜遍4000万医学文献。AI智能推荐,让科研检索更轻松。

立即免费搜索

文件翻译

保留排版,准确专业,支持PDF/Word/PPT等文件格式,支持 12+语言互译。

免费翻译文档

深度研究

AI帮你快速写综述,25分钟生成高质量综述,智能提取关键信息,辅助科研写作。

立即免费体验