Abstract

The availability of a high molecular weight poly(L-lactide), with supposed good mechanical properties, encouraged us to carry out an in vivo experimental study to evaluate the degradation rate and accompanying loss of strength during interaction with bone. Small cylindrical PLLA rods were manufactured by compression moulding. Thirty-six male New Zealand rabbits (b.w. 3 kg), randomly divided into six groups of six animals each, were submitted to implantation of the rods under general anaesthesia (phi 3 x 7 mm rods in the lateral condylic region of the right femur and phi 3 x 50 mm rods in the intracondylic channel of the left femur). The animals were then sacrificed at the end of each experimental time (4, 8, 12, 24, 52, 64 weeks), hence the femurs were explanted. Histology showed no inflammatory cells with fragmentation or resorption of bone trabeculae. Mechanical studies showed a decrease in mechanical properties and flexional stiffness, and the absence of evident material resorption. Finally, the properties of this newly developed resorbable device, when confirmed, seem to justify future clinical introduction of this synthetic material.

摘要

一种具有良好机械性能的高分子量聚(L-丙交酯)的可得性,促使我们开展一项体内实验研究,以评估其在与骨相互作用过程中的降解速率及伴随的强度损失。通过压缩模塑制造出小圆柱形聚左旋乳酸(PLLA)棒。将36只雄性新西兰兔(体重3千克)随机分为6组,每组6只,在全身麻醉下植入这些棒(右股骨外侧髁区域植入直径3×7毫米的棒,左股骨髁间通道植入直径3×50毫米的棒)。然后在每个实验时间点(4、8、12、24、52、64周)结束时处死动物,取出股骨。组织学检查显示无炎性细胞,骨小梁无断裂或吸收。力学研究表明力学性能和弯曲刚度降低,且无明显的材料吸收。最后,这种新开发的可吸收装置的性能一旦得到证实,似乎可为这种合成材料未来的临床应用提供依据。