Abstract

PURPOSE

To evaluate the in vitro secondary caries inhibitory effect of two resin-modified glass ionomer cements (R-GICs).

MATERIALS AND METHODS

Class V cavities were prepared at the cementoenamel junction on facial and lingual surfaces of 32 extracted upper premolars. The facial cavities were restored with a conventional glass ionomer cement (GIC) (Fuji II), while the lingual cavities were restored with either one of the R-GICs (Fuji II LC, Photac Fil, Vitremer), or a resin composite (Z-100). The margins of the restorations were subjected to a 20-day in vitro cariogenic challenge and the degree of demineralization was analyzed by microradiography. The amounts of fluoride released into distilled water from disc specimens of the materials tested were also measured for immersion time up to 161 days.

RESULTS

The R-GICs and GIC's released similar cumulative amounts of fluoride over 161 days. Photac-Fil showed significantly higher amounts of fluoride release over the same period. The depth of the outer lesion and the thickness of the acid-resistant layer showed no significant difference among the R-GICs and GIC's. Moreover, the residual fluoride and calcium in the dentin adjacent to the R-GICs and GIC's were correlated with the thickness of acid-resistant layers in the dentin adjacent to the R-GICs and GIC's by electron probe microanalysis. However, the inhibitory effect of the R-GICs was not directly related to the fluoride concentrations eluted from them.

摘要

目的

评估两种树脂改性玻璃离子水门汀(R - GICs)的体外继发龋抑制效果。

材料与方法

在32颗拔除的上颌前磨牙的颊面和舌面的牙骨质釉质界处制备V类洞。颊面洞用传统玻璃离子水门汀(GIC)(富士II型)修复,而舌面洞用其中一种R - GICs(富士II LC型、Photac Fil型、Vitremer型)或树脂复合材料(Z - 100)修复。修复体边缘接受为期20天的体外致龋挑战,并通过显微放射照相术分析脱矿程度。还测量了测试材料的圆盘标本在长达161天的浸泡时间内释放到蒸馏水中的氟化物量。

结果

在161天内,R - GICs和GIC释放的氟化物累积量相似。在同一时期,Photac - Fil型显示出显著更高的氟化物释放量。R - GICs和GICs之间的外层病变深度和耐酸层厚度没有显著差异。此外,通过电子探针微分析,与R - GICs和GICs相邻的牙本质中的残余氟化物和钙与与R - GICs和GICs相邻的牙本质中的耐酸层厚度相关。然而,R - GICs的抑制作用与从它们中洗脱的氟化物浓度没有直接关系。