Synthesis and characterization of chitosan-poly(acrylic acid) nanoparticles.

作者信息

Hu Yong, Jiang Xiqun, Ding Yin, Ge Haixiong, Yuan Yuyan, Yang Changzheng

机构信息

Department of Polymer Science and Engineering, College of Chemistry and Chemical Engineering, Nanjing University, People's Republic of China.

出版信息

Biomaterials. 2002 Aug;23(15):3193-201. doi: 10.1016/s0142-9612(02)00071-6.

Abstract

Chitosan (CS)-poly(acrylic acid) (PAA) complex nanoparticles, which are well dispersed and stable in aqueous solution, have been prepared by template polymerization of acrylic acid (AA) in chitosan solution. The physicochemical properties of nanoparticles were investigated by using size exclusion chromatography, FT-IR, dynamic light scattering, transmission electron microscope and zeta potential. It was found that the molecular weight of PAA in nanoparticles increased with the increase of molecular weight of CS, indicating that the polymerization of acrylic acid in the chitosan solution was a template polymerization. It was also found that the prepared nanoparticles carried a positive charge and showed the size in the range from 50 to 400 nm. The surface structure and zeta potential of nanoparticles can be controlled by different preparation processes. The experiment of in vitro silk peptide (SP) release showed that these nanoparticles provided a continuous release of the entrapped SP for 10 days, and the release behavior was influenced by the pH value of the medium.

摘要

壳聚糖(CS)-聚丙烯酸(PAA)复合纳米粒子在水溶液中分散良好且稳定,通过在壳聚糖溶液中对丙烯酸(AA)进行模板聚合制备而成。采用尺寸排阻色谱、傅里叶变换红外光谱、动态光散射、透射电子显微镜和zeta电位对纳米粒子的物理化学性质进行了研究。结果发现,纳米粒子中PAA的分子量随CS分子量的增加而增加,这表明壳聚糖溶液中丙烯酸的聚合是一种模板聚合。还发现所制备的纳米粒子带正电荷,尺寸在50至400nm范围内。纳米粒子的表面结构和zeta电位可通过不同的制备工艺进行控制。体外丝素肽(SP)释放实验表明,这些纳米粒子能使包封的SP持续释放10天,且释放行为受介质pH值的影响。