磷酸钙骨水泥粘度的离子改性。第一部分:皮下注射及磷灰石骨水泥强度的提高。

Ionic modification of calcium phosphate cement viscosity. Part I: hypodermic injection and strength improvement of apatite cement.

作者信息

Gbureck Uwe, Barralet Jake E, Spatz Kerstin, Grover Liam M, Thull Roger

机构信息

Department for Functional Materials in Medicine and Dentistry, University of Wuerzburg, Pleicherwall 2, D17 97070 Würzburg, Germany.

出版信息

Biomaterials. 2004 May;25(11):2187-95. doi: 10.1016/j.biomaterials.2003.08.066.

Abstract

A broadening of the indications for which calcium phosphate cements (CPC) can be used, for example, in the field of vertebroplasty, would require injectable and higher strength materials. Unmodified CPC are not injectable due to a filter-pressing effect during injection. In this work we demonstrated that an effective method for improving the injection properties of CPC was by the use of sodium citrate solution as a liquid component. Cement consisting of tetracalcium phosphate (TTCP) and monetite (DCPA) mixed with water up to a powder:liquid ratio (P:L) of 3.3 g/ml had an injectability of approximately 60%. The use of 500 mM trisodium citrate solution instead of water decreased the viscosity of the cement paste to a point, where complete injectability (>95%) through an 800 microm diameter hypodermic needle could be achieved at low loads. The reduction in water demand of the cement effected by the use of sodium citrate enabled high P:L mixes to be formed which were 400% stronger than cements made with water. The effect was less pronounced with compacted cements such that at 9 MPa applied pressure, 58% improvement was obtained and at 50 MPa 36% improvement was measured yielding a cement with a compressive strength of 154 MPa. The liquefying effect of sodium citrate was thought to derive from a strong increase in the surface charge of both the reactants and the product as determined by zeta-potential measurement.

摘要

扩大磷酸钙骨水泥(CPC)的适用范围,例如在椎体成形术领域,将需要可注射且强度更高的材料。未改性的CPC由于注射过程中的压滤效应而不可注射。在这项工作中,我们证明了一种改善CPC注射性能的有效方法是使用柠檬酸钠溶液作为液体成分。由磷酸四钙(TTCP)和磷酸二氢钙(DCPA)组成的骨水泥与水混合,粉末与液体的比例(P:L)为3.3 g/ml时,其可注射性约为60%。使用500 mM柠檬酸钠溶液代替水可将水泥浆的粘度降低到一定程度,在低负荷下通过800微米直径的皮下注射针可实现完全可注射性(>95%)。使用柠檬酸钠降低了骨水泥的需水量,使得能够形成高P:L混合物,其强度比用水制成的骨水泥高400%。对于压实骨水泥,这种效果不太明显,在9 MPa的施加压力下,强度提高了58%,在50 MPa下,强度提高了36%,得到了一种抗压强度为154 MPa的骨水泥。柠檬酸钠的液化作用被认为源于通过zeta电位测量确定的反应物和产物表面电荷的强烈增加。