Dhert W J, Klein C P, Wolke J G, van der Velde E A, de Groot K, Rozing P M
Department of Biomaterials, School of Medicine, University of Leiden, The Netherlands.
J Biomed Mater Res. 1991 Oct;25(10):1183-200. doi: 10.1002/jbm.820251002.
Ceramic coatings of fluorapatite (FA), magnesiumwhitlockite (MW), and hydroxylapatite (HA), and noncoated Ti-6Al-4V alloy (Ti) implants were evaluated before and after implantation in an animal study. Cylindrical plugs were coated by plasma-spraying with FA, MW, and HA. X-ray-diffraction patterns showed for FA and HA a crystalline and for MW an amorphous-crystalline coating structure. The plugs were implanted into the right femora and left humeri of 16 adult goats. Follow-up periods were 12 and 25 weeks. The in vivo results were evaluated using push-out tests and scanning electron microscopy. There were significant differences in push-out strengths between femur and humerus. The FA and HA implants showed significantly higher push-out strengths than the MW and Ti alloy implants, especially for the 12 week follow-up period. Furthermore, at 12 weeks, MW showed significantly lower push-out strengths than Ti alloy. SEM-investigation of the interfaces revealed that FA did not degrade while both MW and HA showed extensive degradation at 12 and 25 weeks. In addition, the interface after push-out testing showed for the MW, HA, and Ti alloy implants to be fractured at the implant-tissue interface and for the FA to be fractured at the coating-titanium interface.
在一项动物研究中,对植入前后的氟磷灰石(FA)、镁白磷钙石(MW)和羟基磷灰石(HA)陶瓷涂层以及未涂层的Ti-6Al-4V合金(Ti)植入物进行了评估。通过等离子喷涂用FA、MW和HA对圆柱形栓体进行涂层。X射线衍射图谱显示,FA和HA为晶体涂层结构,MW为非晶-晶体涂层结构。将栓体植入16只成年山羊的右股骨和左肱骨中。随访期为12周和25周。使用推出试验和扫描电子显微镜对体内结果进行评估。股骨和肱骨的推出强度存在显著差异。FA和HA植入物的推出强度明显高于MW和Ti合金植入物,尤其是在12周的随访期。此外,在12周时,MW的推出强度明显低于Ti合金。对界面的扫描电子显微镜研究表明,FA没有降解,而MW和HA在12周和25周时均显示出广泛降解。此外,推出试验后的界面显示,MW、HA和Ti合金植入物在植入物-组织界面处断裂,而FA在涂层-钛界面处断裂。