Faculty of Dentistry, University of Salamanca, Salamanca, Spain.
Med Oral Patol Oral Cir Bucal. 2010 Jan 1;15(1):e112-8. doi: 10.4317/medoral.15.e112.
To evaluate the effectiveness in the formation of resin tags, adhesive lateral branches and hybrid layers of five adhesive systems, when bonding to dentine.
Flat dentin surfaces from 25 molars were bonded with several adhesive systems according to the manufacturers' instructions. Composite build-ups were constructed incrementally with Tetric Ceram. The Specimens were sectioned parallel to the long axis. One section was treated with phosphoric acid and sodium hypochlorite in order to reveal the hybrid layer formation. The other section was stored in 30% hydrochloric acid to detect resin tags and adhesive lateral branch formation.
The two etch-and-rinse self-priming adhesives exhibited thicker hybrid layers than those found in self-etching adhesive systems. The all-in-one adhesive showed droplet formation between the adhesive and the resin composite. The resin tags formed with the etch-and-rinse adhesives were much longer than those found with the self-etching adhesives. Lateral branch formation was observed in etch-and-rinse adhesives and in one of the self-etch adhesives Clearfil SE Bond (SEB).
The formed hybrid layer obtained with the two-step self-etching adhesives and the etch-and-rinse systems were continuous and uniform in thickness. Droplets within the all-in-one adhesive layer may occur as a result of water absorption from dentin through osmosis, and may interfere with proper resin polymerization. Resin tags obtained with SEB and the etch-and-rinse adhesive systems showed lateral branches, which is a sign of proper resin infiltration.
评估 5 种粘接系统在牙本质粘接时形成树脂标签、粘接侧枝和混合层的效果。
从 25 颗磨牙上获得平坦的牙本质表面,根据制造商的说明用几种粘接系统进行粘接。用 Tetric Ceram 分层构建复合层。将标本沿长轴平行切割。一部分用磷酸和次氯酸钠处理以显示混合层的形成。另一部分储存在 30%盐酸中以检测树脂标签和粘接侧枝的形成。
两种酸蚀自酸蚀自启动粘接剂的混合层比自酸蚀粘接系统发现的混合层厚。一体化粘接剂在粘接剂和树脂复合材料之间形成液滴。酸蚀自酸蚀粘接剂形成的树脂标签比自酸蚀粘接剂形成的树脂标签长很多。在酸蚀自酸蚀粘接剂和一种自酸蚀粘接剂 Clearfil SE Bond (SEB) 中观察到侧枝形成。
两步自酸蚀粘接剂和酸蚀自酸蚀系统形成的混合层连续且厚度均匀。一体化粘接剂层内的液滴可能是由于渗透作用从牙本质吸收水分引起的,可能会干扰适当的树脂聚合。SEB 和酸蚀自酸蚀粘接剂系统形成的树脂标签显示出侧枝,这是适当的树脂渗透的标志。