Abstract

The aim of this study was to evaluate the influence of different surface treatments (air abrasion, acid etching, and laser irradiation) on the surface roughness and bond strength of a low fusing ceramic. Thirty-six discs of low fusing ceramic (Finesse, Ceramco) were prepared (10 mm in diameter and 2 mm in thickness) according to the manufacturer's instructions. Specimens were divided into three groups (n = 12), and the following treatments were performed: Air abrasion with alumina particles (50 μm), acid etching with 5% HF and Nd:YAG laser irradiation (distance: 1 mm, 100 mJ, 20 Hz, 2 W, and 141.54 J/cm(2)). Following determination of surface roughness (R(a)) by profilometry, specimens were examined with scanning electron microscopy (SEM). The luting cement (Clearfil Esthetic Cement) was bonded to the ceramic specimens using Teflon tubes. After 24 h of water storage, shear bond strength test was performed using a universal testing machine at a crosshead speed of 1 mm/min. The data were analyzed with two-way analysis of variance (ANOVA) and Tukey HSD tests (α = .05). Two-way ANOVA indicated that surface roughness was significantly affected by surface treatments (p < .001). Tukey honestly significant difference (HSD) indicated that the air abrasion group had a significantly higher mean value (p < .05) than the other groups. Shear bond strength was significantly affected by surface treatments (p < .001). Tukey HSD indicated that the air abrasion group had a significantly higher mean value (p < .05) than the other groups. No significant difference was found between the acid-etching and laser-irradiation groups (p > .05). The SEM image of the laser irradiation surface appeared to be relatively smooth as compared to the images of other the groups. Air abrasion of low-fusing porcelain surfaces was effective in improving the bond strength as compared to the acid-etching and laser-irradiation methods.

摘要

本研究旨在评估不同表面处理(喷砂、酸蚀和激光照射)对低熔陶瓷表面粗糙度和结合强度的影响。根据制造商的说明,制备了 36 个低熔陶瓷(Finesse, Ceramco)圆盘(直径 10mm,厚度 2mm)。将标本分为三组(n=12),并进行以下处理:用氧化铝颗粒喷砂、用 5%HF 酸蚀和 Nd:YAG 激光照射(距离:1mm,100mJ,20Hz,2W,141.54J/cm²)。通过轮廓仪测定表面粗糙度(Ra)后,用扫描电子显微镜(SEM)观察标本。用聚四氟乙烯管将粘结剂(Clearfil Esthetic Cement)粘接到陶瓷标本上。水储存 24 小时后,用万能试验机以 1mm/min 的十字头速度进行剪切结合强度测试。使用双因素方差分析(ANOVA)和 Tukey HSD 检验(α=0.05)对数据进行分析。双因素 ANOVA 表明,表面粗糙度受到表面处理的显著影响(p<0.001)。Tukey 诚实显著差异(HSD)表明,喷砂组的平均值显著高于其他组(p<0.05)。剪切结合强度受到表面处理的显著影响(p<0.001)。Tukey HSD 表明,喷砂组的平均值显著高于其他组(p<0.05)。酸蚀组和激光照射组之间没有显著差异(p>0.05)。与其他组相比,激光照射表面的 SEM 图像似乎相对较光滑。与酸蚀和激光照射方法相比,低熔瓷表面的喷砂处理能有效提高结合强度。

文献AI研究员

20分钟写一篇综述,助力文献阅读效率提升50倍。

立即体验

用中文搜PubMed

大模型驱动的PubMed中文搜索引擎

马上搜索

文档翻译

学术文献翻译模型,支持多种主流文档格式。

立即体验