Department of Biology Science, Bauru School of Dentistry, University of São Paulo, Bauru, SP, Brazil.
J Appl Oral Sci. 2010 Sep-Oct;18(5):461-6. doi: 10.1590/s1678-77572010000500006.
This in vitro study evaluated the cytotoxicity of an experimental restorative composite resin subjected to different light-curing regimens.
Forty round-shaped specimens were prepared and randomly assigned to four experimental groups (n=10), as follows: in Group 1, no light-curing; in Groups 2, 3 and 4, the composite resin specimens were light-cured for 20, 40 or 60 s, respectively. In Group 5, filter paper discs soaked in 5 µL PBS were used as negative controls. The resin specimens and paper discs were placed in wells of 24-well plates in which the odontoblast-like cells MDPC-23 (30,000 cells/cm²) were plated and incubated in a humidified incubator with 5% CO2 and 95% air at 37ºC for 72 h. The cytotoxicity was evaluated by the cell metabolism (MTT assay) and cell morphology (SEM). The data were analyzed statistically by Kruskal-Wallis and Mann-Whitney tests (p<0.05).
In G1, cell metabolism decreased by 86.2%, indicating a severe cytotoxicity of the non-light-cured composite resin. On the other hand, cell metabolism decreased by only 13.3% and 13.5% in G2 and G3, respectively. No cytotoxic effects were observed in G4 and G5. In G1, only a few round-shaped cells with short processes on their cytoplasmic membrane were observed. In the other experimental groups as well as in control group, a number of spindle-shaped cells with long cytoplasmic processes were found.
Regardless of the photoactivation time used in the present investigation, the experimental composite resin presented mild to no toxic effects to the odontoblast-like MDPC-23 cells. However, intense cytotoxic effects occurred when no light-curing was performed.
本体外研究评估了一种实验性修复复合树脂在不同光固化方案下的细胞毒性。
制备 40 个圆形试件,并随机分为 4 个实验组(n=10),如下:组 1,不进行光固化;组 2、3 和 4 分别对复合树脂试件进行 20、40 或 60 s 的光固化。在组 5 中,使用浸泡在 5 µL PBS 中的滤纸盘作为阴性对照。将树脂试件和滤纸盘放置在 24 孔板的孔中,在孔中接种了类似成牙本质细胞的 MDPC-23(30,000 个细胞/cm²),并在 37°C 、5%CO2 和 95%空气的加湿孵育箱中孵育 72 h。通过细胞代谢(MTT 测定)和细胞形态(SEM)评估细胞毒性。使用 Kruskal-Wallis 和 Mann-Whitney 检验对数据进行统计学分析(p<0.05)。
在 G1 组中,细胞代谢降低了 86.2%,表明未光固化的复合树脂具有严重的细胞毒性。另一方面,在 G2 和 G3 组中,细胞代谢分别仅降低了 13.3%和 13.5%。在 G4 和 G5 组中未观察到细胞毒性作用。在 G1 组中,仅观察到少数细胞膜上具有短突起的圆形细胞。在其他实验组以及对照组中,发现了许多具有长细胞质突起的梭形细胞。
无论在本研究中使用哪种光激活时间,实验性复合树脂对类似成牙本质细胞的 MDPC-23 细胞均表现出轻度至无毒性作用。然而,当不进行光固化时,则会发生强烈的细胞毒性作用。