瓷贴面修复体长达 20 年的临床效果。

Clinical performance of porcelain laminate veneers for up to 20 years.

机构信息

Clinical Department of Restorative and Prosthetics Dentistry, Innsbruck Medical University, Austria.

出版信息

Int J Prosthodont. 2012 Jan-Feb;25(1):79-85.

Abstract

PURPOSE

The aim of this clinical retrospective study was to evaluate the clinical quality, success rate, and estimated survival rate of anterior veneers made of silicate glass-ceramic in a long-term analysis of up to 20 years.

MATERIALS AND METHODS

Anterior teeth in the maxillae and mandibles of 84 patients (38 men, 46 women) were restored with 318 porcelain veneer restorations between 1987 and 2009 at the Medical University Innsbruck, Innsbruck, Austria. Clinical examination was performed during patients' regularly scheduled maintenance appointments. Esthetic match, porcelain surface, marginal discoloration, and integrity were evaluated following modified California Dental Association/Ryge criteria. Veneer failures and reasons for failure were recorded. The study population included 42 (50.0%) patients diagnosed with bruxism and 23 (27.38%) smokers. The success rate was determined using Kaplan-Meier survival analysis.

RESULTS

The mean observation time was 118 ± 63 months. Twenty-nine failures (absolute: 82.76%, relative: 17.24%) were recorded. The main reason for failure was fracture of the ceramic (44.83%). The estimated survival rate was 94.4% after 5 years, 93.5% at 10 years, and 82.93% at 20 years. Nonvital teeth showed a significantly higher failure risk (P = .0012). There was a 7.7-times greater risk of failure associated with existing parafunction (bruxism, P = .0004). Marginal discoloration was significantly greater in smokers (P ⋜ .01).

CONCLUSION

Porcelain laminate veneers offer a predictable and successful restoration with an estimated survival probability of 93.5% over 10 years. Significantly increased failure rates were associated with bruxism and nonvital teeth, and marginal discoloration was worse in patients who smoked.

摘要

目的

本临床回顾性研究旨在评估长达 20 年的长期分析中,硅酸锂玻璃陶瓷制作的前牙贴面的临床质量、成功率和估计存活率。

材料和方法

1987 年至 2009 年期间,在奥地利因斯布鲁克医科大学,对 84 名患者(38 名男性,46 名女性)的上颌和下颌前牙进行了 318 个瓷贴面修复。临床检查在患者定期进行的维护预约期间进行。根据改良的加利福尼亚牙科协会/里格标准评估美学匹配、瓷面、边缘变色和完整性。记录贴面失败和失败原因。研究人群包括 42 名(50.0%)被诊断为磨牙症的患者和 23 名(27.38%)吸烟者。使用 Kaplan-Meier 生存分析确定成功率。

结果

平均观察时间为 118 ± 63 个月。记录了 29 次失败(绝对:82.76%,相对:17.24%)。主要失败原因是陶瓷断裂(44.83%)。5 年后估计生存率为 94.4%,10 年后为 93.5%,20 年后为 82.93%。非活髓牙的失败风险显著增加(P =.0012)。存在磨牙症等异常功能(P =.0004),失败风险增加 7.7 倍。吸烟者的边缘变色明显更大(P ⋜.01)。

结论

瓷层压贴面提供了一种可预测且成功的修复方法,10 年内的估计生存率为 93.5%。磨牙症和非活髓牙与显著增加的失败率相关,吸烟者的边缘变色更差。