Schoen F J, Tsao J W, Levy R J
Am J Pathol. 1986 Apr;123(1):134-45.
Calcification of bioprosthetic heart valves fabricated from glutaraldehyde-pretreated bovine pericardium has not been investigated. The objectives of this study were to characterize pericardium before and after glutaraldehyde pretreatment and to study the pathophysiology of mineralization of glutaraldehyde-preserved pericardium. Pericardial protein was approximately 90% collagen, predominantly Type I. Glutaraldehyde incorporation was complete following 24 hours' incubation (151 X 10(-9) mol/mg). Bovine pericardium pretreated in buffered 0.6% glutaraldehyde, implanted subcutaneously in young rats for 24 hours to 112 days, was analyzed chemically (calcium and phosphorus) and morphologically. Mineralization, detected at 48 hours' implantation, was initially associated with pericardial connective tissue cells and later also collagen. Mean calcium content was 114 micrograms/mg at 21 days and 199 micrograms/mg at 112 days. The morphologic features and the kinetics and degree of mineral accumulation in glutaraldehyde-pretreated bovine pericardium were strikingly similar to those previously determined for porcine aortic valve. These results predict that calcification will critically limit the late durability of clinical pericardial bioprostheses and suggest generalized mechanisms of bioprosthetic tissue mineralization which are probably dependent on modification of implant microstructure by glutaraldehyde pretreatment.
由戊二醛预处理牛心包制成的生物人工心脏瓣膜的钙化情况尚未得到研究。本研究的目的是表征戊二醛预处理前后的心包,并研究戊二醛保存心包矿化的病理生理学。心包蛋白约90%为胶原蛋白,主要是I型。孵育24小时后戊二醛掺入完成(151×10⁻⁹摩尔/毫克)。将在缓冲的0.6%戊二醛中预处理的牛心包皮下植入幼鼠24小时至112天,进行化学分析(钙和磷)和形态学分析。植入48小时时检测到矿化,最初与心包结缔组织细胞有关,后来也与胶原蛋白有关。21天时平均钙含量为114微克/毫克,112天时为199微克/毫克。戊二醛预处理牛心包的形态学特征、矿物质积累的动力学和程度与先前对猪主动脉瓣测定的结果惊人地相似。这些结果预测钙化将严重限制临床心包生物人工瓣膜的后期耐久性,并提示生物人工组织矿化的一般机制,这可能取决于戊二醛预处理对植入物微观结构的改变。