Suppr超能文献

树脂粘结水门汀与玻璃陶瓷材料之间的粘结情况

Aspects of bonding between resin luting cements and glass ceramic materials.

作者信息

Tian Tian, Tsoi James Kit-Hon, Matinlinna Jukka P, Burrow Michael F

机构信息

Oral Diagnosis and Polyclinics, Faculty of Dentistry, University of Hong Kong, Prince Philip Dental Hospital, Hong Kong.

Dental Materials Science, Faculty of Dentistry, University of Hong Kong, Hong Kong.

出版信息

Dent Mater. 2014 Jul;30(7):e147-62. doi: 10.1016/j.dental.2014.01.017. Epub 2014 Mar 6.

Abstract

OBJECTIVES

The bonding interface of glass ceramics and resin luting cements plays an important role in the long-term durability of ceramic restorations. The purpose of this systematic review is to discuss the various factors involved with the bond between glass ceramics and resin luting cements.

METHODS

An electronic Pubmed, Medline and Embase search was conducted to obtain laboratory studies on resin-ceramic bonding published in English and Chinese between 1972 and 2012.

RESULTS AND DISCUSSION

Eighty-three articles were included in this review. Various factors that have a possible impact on the bond between glass ceramics and resin cements were discussed, including ceramic type, ceramic crystal structure, resin luting cements, light curing, surface treatments, and laboratory test methodology.

CONCLUSIONS

Resin-ceramic bonding has been improved substantially in the past few years. Hydrofluoric acid (HF) etching followed by silanizaiton has become the most widely accepted surface treatment for glass ceramics. However, further studies need to be undertaken to improve surface preparations without HF because of its toxicity. Laboratory test methods are also required to better simulate the actual oral environment for more clinically compatible testing.

摘要

目的

玻璃陶瓷与树脂粘结水门汀的粘结界面在陶瓷修复体的长期耐久性中起着重要作用。本系统评价的目的是探讨与玻璃陶瓷和树脂粘结水门汀之间的粘结相关的各种因素。

方法

进行电子检索,检索1972年至2012年间发表的英文和中文关于树脂-陶瓷粘结的实验室研究,检索数据库包括PubMed、Medline和Embase。

结果与讨论

本评价纳入了83篇文章。讨论了可能影响玻璃陶瓷与树脂水门汀之间粘结的各种因素,包括陶瓷类型、陶瓷晶体结构、树脂粘结水门汀、光固化、表面处理和实验室测试方法。

结论

在过去几年中,树脂-陶瓷粘结已得到显著改善。氢氟酸(HF)蚀刻后进行硅烷化已成为玻璃陶瓷最广泛接受的表面处理方法。然而,由于HF的毒性,需要进行进一步研究以改进无HF的表面处理方法。还需要实验室测试方法来更好地模拟实际口腔环境,以进行更符合临床的测试。