J Environ Manage. 2018 Feb 15;208:15-23. doi: 10.1016/j.jenvman.2017.11.071. Epub 2017 Dec 12.
The leaching behavior of six typical toxic metals (Pb, Zn, Cr, Cd, Cu and Ni) from raw and chemically stabilized (phosphate and chelating agent) municipal solid waste incineration (MSWI) fly ash were investigated using citric acid. Leaching tests indicated that phosphate stabilization can effectively decrease the leaching of Zn, Cd and Cr; whereas chelating agent stabilization shows a strong ability to lower the release of Pb, Cd and Cu, but instead increases the solubility of Zn and Cr at low pH conditions. Sequential extraction results suggested that the leaching of Pb, Zn and Cd in both the stabilized MSWI fly ash samples led to the decrease in Fe/Mn oxide fraction and the increase in exchangeable and carbonate fractions. The leaching of Cr was due to the decrease in exchangeable, carbonate and Fe/Mn oxide fractions in phosphate-stabilized and chelating agent-stabilized MSWI fly ash. The leaching of Cu in both stabilized MSWI fly ash was greatly ascribed to the decrease in Fe/Mn oxide and oxidisable fractions. Moreover, predicted curves by geochemical model indicated that both stabilized MSWI fly ash have the risk of releasing toxic metals under strong acid environment.
采用柠檬酸对原生和化学稳定化(磷酸盐和螯合剂)城市固体废弃物焚烧飞灰中 6 种典型有毒金属(Pb、Zn、Cr、Cd、Cu 和 Ni)的浸出行为进行了研究。浸出试验表明,磷酸盐稳定化可有效降低 Zn、Cd 和 Cr 的浸出率;而螯合剂稳定化则表现出较强的降低 Pb、Cd 和 Cu 释放能力,但在低 pH 条件下会增加 Zn 和 Cr 的溶解度。顺序提取结果表明,两种稳定化 MSWI 飞灰样品中 Pb、Zn 和 Cd 的浸出导致 Fe/Mn 氧化物相减少,可交换相和碳酸盐相增加。磷酸盐稳定化和螯合剂稳定化 MSWI 飞灰中 Cr 的浸出归因于可交换相、碳酸盐相和 Fe/Mn 氧化物相的减少。此外,地球化学模型预测曲线表明,在强酸环境下,两种稳定化 MSWI 飞灰均有释放有毒金属的风险。