J Med Life. 2022 Apr;15(4):448-453. doi: 10.25122/jml-2020-0104.
This study aimed to compare the effect of 4 different intracanal medicaments on the push-out bond strength of two sealers (AH Plus and MTA Fillapex). 100 single-rooted extracted premolar teeth were divided into 5 groups, with 20 samples in each group, one group being the control group. After cleaning and shaping procedures, the canals were filled with 4 different medicaments: calcium hydroxide, tri-antibiotic paste (TAP), Metapex, or Chlorhexidine (2%) gel for 2 weeks. Following this, the medicaments were rinsed away, and the samples in those sub-groups were obturated with gutta-percha/AH Plus or MTA Fillapex sealers. After 2 weeks of incubation, a 2-mm-thick middle section from each root was evaluated to test push-out strength. The obtained data were tabulated, and appropriate statistical analysis was performed (two-way ANOVA and LSD test). When comparing the average values, the bond strength values of AH Plus were significantly higher than those of MTA Fillapex (p<0.05) in all medicament groups. Based on the findings, we concluded that AH Plus had comparatively higher bond strength than MTA Fillapex. We also observed that AH Plus had higher bond strength in the presence of calcium hydroxide, whereas MTA Fillapex in the presence of Chlorhexidine. A comparison of the push-out bond strength shows that irrespective of the root canal segment or the final irrigant used, AH Plus showed higher values among all groups. The limitation of the current study was that the effect of TAP on the bond strength of endodontic sealers was not negative.
本研究旨在比较 4 种不同根管内药物对 2 种封闭剂(AH Plus 和 MTA Fillapex)的推出粘结强度的影响。100 颗单根前磨牙随机分为 5 组,每组 20 颗,1 组为对照组。在根管清洗和成形后,用 4 种不同的药物填充根管:氢氧化钙、三抗生素糊剂(TAP)、Metapex 或洗必泰(2%)凝胶,持续 2 周。然后,冲洗掉药物,将这些亚组的样本用牙胶/AH Plus 或 MTA Fillapex 封闭剂封闭。2 周孵育后,从每个根的中间部位切取 2mm 厚的中间部分,以测试推出强度。将获得的数据制表,并进行适当的统计分析(双因素方差分析和 LSD 检验)。在比较平均值时,在所有药物组中,AH Plus 的粘结强度均显著高于 MTA Fillapex(p<0.05)。基于这些发现,我们得出结论,AH Plus 的粘结强度比 MTA Fillapex 高。我们还观察到,在存在氢氧化钙的情况下,AH Plus 的粘结强度更高,而在存在洗必泰的情况下,MTA Fillapex 的粘结强度更高。对推出粘结强度的比较表明,无论根管段或最终冲洗液如何,AH Plus 在所有组中均显示出更高的数值。本研究的局限性在于 TAP 对根管封闭剂粘结强度的影响并不为负。