Suppr超能文献

金、锂硅氧体、透锂长石和间接树脂复合材料制作的牙冠内修复体的临床寿命:系统评价和荟萃分析。

Clinical longevity of intracoronal restorations made of gold, lithium disilicate, leucite, and indirect resin composite: a systematic review and meta-analysis.

机构信息

Department of Restorative Dentistry and Biomaterials, Center for Dentistry and Oral Hygiene, University Medical Center Groningen, University of Groningen, Antonius Deusinglaan 1, 9713 AV, Groningen, The Netherlands.

Department of Epidemiology, University Medical Center Groningen, University of Groningen, Groningen, The Netherlands.

出版信息

Clin Oral Investig. 2023 Sep;27(9):4877-4896. doi: 10.1007/s00784-023-05050-x. Epub 2023 Aug 19.

Abstract

OBJECTIVES

The aim of this systematic review and meta-analysis is to assess the comparative clinical success and survival of intracoronal indirect restorations using gold, lithium disilicate, leucite, and indirect composite materials.

MATERIAL AND METHODS

This systematic review and meta-analysis were conducted following the Cochrane Handbook for Systematic Reviews of Interventions and PRISMA guidelines. The protocol for this study was registered in PROSPERO (registration number: CRD42021233185). A comprehensive literature search was conducted across various databases and sources, including PubMed/Medline, Embase, Cochrane Library, Web of Science, ClinicalTrials.gov, and gray literature. A total of 7826 articles were screened on title and abstract. Articles were not excluded based on the vitality of teeth, the language of the study, or the observation period. The risk difference was utilized for the analyses, and a random-effects model was applied. All analyses were conducted with a 95% confidence interval (95% CI). The calculated risk differences were derived from the combined data on restoration survival and failures obtained from each individual article. The presence of heterogeneity was assessed using the I statistic, and if present, the heterogeneity of the data in the articles was evaluated using the non-parametric chi-squared statistic (p < 0.05).

RESULTS

A total of 12 eligible studies were selected, which included 946 restorations evaluated over a minimum observation period of 1 year and a maximum observation period of 7 years. Results of the meta-analysis indicated that intracoronal indirect resin composite restorations have an 18% higher rate of failure when compared to intracoronal gold restorations over 5-7 years of clinical service (risk difference =  - 0.18 [95% CI: - 0.27, - 0.09]; p = .0002; I = 0%). The meta-analysis examining the disparity in survival rates between intracoronal gold and leucite restorations could not be carried out due to methodological differences in the studies.

CONCLUSIONS

According to the currently available evidence, medium-quality data indicates that lithium disilicate and indirect composite materials demonstrate comparable survival rates in short-term follow-up. Furthermore, intracoronal gold restorations showed significantly higher survival rates, making them a preferred option over intracoronal indirect resin-composite restorations. Besides that, the analysis revealed no statistically significant difference in survival rates between leucite and indirect composite restorations. The short observation period, limited number of eligible articles, and low sample size of the included studies were significant limitations.

CLINICAL SIGNIFICANCE

Bearing in mind the limitations of the reviewed literature, this systematic review and meta-analysis help clinicians make evidence-based decisions on how to restore biomechanically compromised posterior teeth.

摘要

目的

本系统评价和荟萃分析的目的是评估使用金、锂硅、白榴石和间接复合材料进行牙内间接修复的临床成功率和存活率。

材料和方法

本系统评价和荟萃分析遵循 Cochrane 干预系统评价手册和 PRISMA 指南进行。本研究的方案已在 PROSPERO(注册号:CRD42021233185)中注册。对各种数据库和来源(包括 PubMed/Medline、Embase、Cochrane 图书馆、Web of Science、ClinicalTrials.gov 和灰色文献)进行了全面的文献检索。在标题和摘要层面共筛选了 7826 篇文章。未根据牙齿活力、研究语言或观察期排除文章。采用风险差异进行分析,并应用随机效应模型。所有分析均采用 95%置信区间(95%CI)。从每个单独文章中获得的修复体存活和失败的综合数据中得出计算的风险差异。使用 I 统计量评估异质性的存在,如果存在,则使用非参数卡方统计量(p<0.05)评估文章中数据的异质性。

结果

共选择了 12 项符合条件的研究,其中包括 946 项修复体,观察期最短为 1 年,最长为 7 年。荟萃分析结果表明,在 5-7 年的临床服务中,牙内间接树脂复合材料修复体的失败率比牙内金修复体高 18%(风险差异=-0.18[95%CI:-0.27,-0.09];p=0.0002;I=0%)。由于研究方法的差异,无法进行牙内金和白榴石修复体存活率差异的荟萃分析。

结论

根据目前的证据,中等质量的数据表明,锂硅和间接复合材料在短期随访中显示出相似的存活率。此外,牙内金修复体显示出更高的存活率,使其成为牙内间接树脂复合材料修复体的首选。此外,分析显示白榴石和间接复合材料修复体的存活率无统计学差异。综述文献的局限性包括观察期短、合格文章数量有限和纳入研究的样本量小。

临床意义

考虑到所审查文献的局限性,本系统评价和荟萃分析有助于临床医生根据如何修复生物力学受损的后牙做出基于证据的决策。

https://cdn.ncbi.nlm.nih.gov/pmc/blobs/2eef/10492736/93804db76b48/784_2023_5050_Fig1_HTML.jpg