Biomaterials Department, Faculty of Dentistry, Ain-Shams University, African Union Organization Street, Abbasia, Cairo, 11566, Egypt.
BMC Oral Health. 2023 Dec 5;23(1):966. doi: 10.1186/s12903-023-03710-8.
The study aimed to evaluate the influence of various beverages; with and without brushing; on the surface mechanical properties of two resin composites.
A total of 160 disc-shaped specimens were prepared for each of the following dental composites; nanohybrid ormocer (Admira fusion, VOCO GmbH, Cuxhaven, Germany) and nanohybrid resin composite (Grandio, VOCO GmbH, Cuxhaven, Germany). The baseline surface hardness and roughness measurements were carried out after 24 h. The composite samples were randomly distributed into one of the two groups; brushing and non-brushing, which were further divided into one of the four subgroups (n = 10); artificial saliva as control, coffee, red wine, and soft drink. In the non-brushing group, the specimens were immersed in the different beverages for five minutes three times daily for 30 days. The same procedure was done for the brushing group, in addition to brushing the specimens for five seconds. The surface hardness and roughness measurements were repeated after 30 days. One-way ANOVA and independent t-tests were used for statistical analysis.
The soft drink had the most deteriorating effect and artificial saliva had the least. The change in surface properties was higher in the brushing subgroups. Grandio exhibited a higher change in surface microhardness while Admira fusion exhibited a higher change in surface roughness.
The surface properties of both dental resin composites were negatively affected by using beverages and brushing.
本研究旨在评估不同饮料(含刷牙和不含刷牙)对两种树脂复合材料表面力学性能的影响。
为以下两种牙科复合材料各制备 160 个圆盘状试件:纳米复合有机硅树脂(Admira fusion,VOCO GmbH,德国库克斯港)和纳米复合树脂复合材料(Grandio,VOCO GmbH,德国库克斯港)。在 24 小时后进行基线表面硬度和粗糙度测量。将复合材料样本随机分为刷牙和不刷牙两组,每组再分为四个亚组(n=10):人工唾液为对照组,咖啡、红酒和软饮料。在不刷牙组中,将标本每天浸泡在不同的饮料中 5 分钟,共 30 天。刷牙组进行相同的程序,此外,还要对标本进行 5 秒的刷牙。在 30 天后重复表面硬度和粗糙度测量。采用单因素方差分析和独立 t 检验进行统计学分析。
软饮料的影响最大,人工唾液的影响最小。刷牙亚组的表面性能变化更高。Grandio 表现出更高的表面显微硬度变化,而 Admira fusion 则表现出更高的表面粗糙度变化。
使用饮料和刷牙会对两种牙科树脂复合材料的表面性能产生负面影响。