Suppr超能文献

不同光活化固化模式照射下牙科复合材料的单体转化率和细胞毒性

Monomer conversion and cytotoxicity of dental composites irradiated with different modes of photoactivated curing.

作者信息

Tseng Wan-Yu, Huang Chien-Hsun, Chen Ruey-Song, Lee Ming-Shu, Chen Yi-Jane, Rueggeberg Frederick A, Chen Min-Huey

机构信息

Graduate Institute of Clinical Dental Science, School of Dentistry, College of Medicine, National Taiwan University, Taipei, Taiwan.

出版信息

J Biomed Mater Res B Appl Biomater. 2007 Oct;83(1):85-90. doi: 10.1002/jbm.b.30769.

Abstract

The aim of the study was to compare the monomer conversion and cytotoxicity of two resin composites, Tetric Ceram (TC) and Heliomolar (HM), irradiated with a halogen light-curing unit (Optilux 501) using a number of curing modes, boost (OB), ramp (OR), and conventional (OC), as well as a light-emitting diode (LED) curing unit (LEDemetron; LEDe). The effects of irradiation times (10, 20, 30, and 40 s) were also investigated. The monomer conversion of resin composites was measured using Fourier transform infrared (FTIR) analysis. Resin samples were preimmersed in Dulbeco's modified engles medium (DMEM) for 24 h, and the periodontal ligament cells (PDL) were cultured with aged medium for 72 h to evaluate the cytotoxic effects of resin samples using the microtiter-tetrazolium (MTT) method. The spectral outputs of the curing units were also compared. After irradiation using the same curing mode, the TC monomer conversion was higher than the HM analog. The TC conversion value was lower after OC and LEDemetron irradiation for 10 s compared to exposures of 30 and 40 s. The HM conversion value was lowest for the 10-s OC irradiation, and highest for the 40-s OC exposure. In cytotoxicity tests, the negative control group was without irradiation. The succinate dehydrogenase (SDH) activities of the OB and OR-irradiated TC samples were significantly lower than analogs irradiated with LEDemetron for 40 s; however, no significant differences were demonstrated between OB, OR, and control groups. Further, no significant differences in SDH activity were demonstrated for OB, OR, and control groups of the HM.

摘要

本研究的目的是比较两种树脂复合材料,即Tetric Ceram(TC)和Heliomolar(HM),在使用多种固化模式(增强固化模式(OB)、斜坡固化模式(OR)和传统固化模式(OC))的卤素光固化机(Optilux 501)以及发光二极管(LED)固化机(LEDemetron;LEDe)照射下的单体转化率和细胞毒性。同时还研究了照射时间(10、20、30和40秒)的影响。使用傅里叶变换红外光谱(FTIR)分析来测量树脂复合材料的单体转化率。将树脂样本预先浸入杜氏改良伊格尔培养基(DMEM)中24小时,然后用老化培养基培养牙周膜细胞(PDL)72小时,以使用微量滴定四氮唑盐(MTT)法评估树脂样本的细胞毒性作用。还比较了固化机的光谱输出。在使用相同固化模式照射后,TC的单体转化率高于HM类似物。与30秒和40秒的照射时间相比,在OC和LEDemetron照射10秒后,TC的转化率较低。HM的转化率在10秒OC照射时最低,在40秒OC照射时最高。在细胞毒性测试中,阴性对照组未进行照射。OB和OR照射的TC样本的琥珀酸脱氢酶(SDH)活性显著低于用LEDemetron照射40秒的类似物;然而,OB、OR和对照组之间未显示出显著差异。此外,HM的OB、OR和对照组在SDH活性方面也未显示出显著差异。