用三聚偏磷酸钠对低氟浓度凝胶进行牙釉质再矿化的原位评估。

In situ evaluation of a low fluoride concentration gel with sodium trimetaphosphate in enamel remineralization.

作者信息

Danelon Marcelle, Takeshita Eliana M, Sassaki Kikue T, Delbem Alberto Carlos Botazzo

机构信息

Department of Pediatric Dentistry, Faculty of Dentistry of Araçatuba, Univ. Estadual Paulista (UNESP), Rua José Bonifácio 1193, Araçatuba, SP - CEP 16015-050, Brazil.

出版信息

Am J Dent. 2013 Feb;26(1):15-20.

Abstract

PURPOSE

To evaluate the capability of gels with low fluoride (F) concentration and supplemented with sodium trimetaphosphate (TMP) to promote in situ enamel remineralization.

METHODS

Bovine enamel blocks were selected on the basis of their surface hardness after demineralization, and divided into five groups: gel without F or TMP (placebo); gel with 4,500 ppm F (4,500); gel with 4,500 ppm F + 5% TMP (4,500 5% TMP); gel with 9,000 ppm F (9,000) and gel with 12,300 ppm F (12,300). The study design was blind and cross-over: 12 subjects used palatal devices with four demineralized enamel blocks for 3 days, after topical fluoride application (TFA). Two blocks were removed immediately for analysis of the loosely bound fluoride (CaF2) and firmly bound fluoride (F) after TFA in enamel. In the remaining blocks, the percentage of surface hardness recovery (% SH), cross-sectional hardness (deltaKHN) and CaF2 and F were determined after remineralization. The results were subjected to ANOVA and Bonferroni tests (P < 0.05).

RESULTS

The groups 4,500 5% TMP, 9,000, and 12,300 showed the best results with regard to % SH (P < 0.05). Lower deltaKHN values were observed in the 4,500 5% TMP and 12,300 gel groups (P < 0.05). Higher concentrations of CaF2 and F were observed in the 12,300 group, followed by the 4,500 5% TMP and 9,000 groups (P > 0.05). It was concluded that it is possible to promote enamel remineralization using gels with low fluoride concentration supplemented with TMP.

摘要

目的

评估低氟浓度并添加三聚偏磷酸钠(TMP)的凝胶促进牙釉质原位再矿化的能力。

方法

根据脱矿后牛牙釉质块的表面硬度进行选择,并分为五组:不含氟或TMP的凝胶(安慰剂);含4500 ppm氟的凝胶(4500);含4500 ppm氟 + 5% TMP的凝胶(4500 5% TMP);含9000 ppm氟的凝胶(9000)和含12300 ppm氟的凝胶(12300)。研究设计为双盲交叉:12名受试者在局部用氟(TFA)后,使用带有四个脱矿牙釉质块的腭部装置3天。立即取出两个牙釉质块,分析TFA后牙釉质中松散结合的氟(CaF2)和牢固结合的氟(F)。在其余的牙釉质块中,再矿化后测定表面硬度恢复百分比(% SH)、横截面硬度(deltaKHN)以及CaF2和F。结果进行方差分析和Bonferroni检验(P < 0.05)。

结果

在% SH方面,4500 5% TMP、9000和12300组显示出最佳结果(P < 0.05)。在4500 5% TMP和12300凝胶组中观察到较低的deltaKHN值(P < 0.05)。在12300组中观察到较高浓度的CaF2和F,其次是4500 5% TMP和9000组(P > 0.05)。得出的结论是,使用添加TMP的低氟浓度凝胶有可能促进牙釉质再矿化。