Manfro Rafael, Fonseca Fabiano Silva, Bortoluzzi Marcelo Carlos, Sendyk Wilson Roberto
Department of Dental Implantology, SOEBRAS, Street Presidente Coutinho 264/903, Florianópolis, SC CEP 88015-230 Brazil.
Vitória, ES Brazil.
J Maxillofac Oral Surg. 2014 Dec;13(4):464-70. doi: 10.1007/s12663-013-0554-z. Epub 2013 Aug 2.
Anorganic bovine xenogenous grafts show the best performance as bone substitutes in implantodontics. Bio-Oss is the world's most widely used and investigated anorganic bone substitute. This article compares two anorganic bovine bone substitutes (Bone-Fill and Gen-Ox anorganic) with Bio-Oss.
Eight New Zealand rabbits were implanted with 4 titanium cylinders randomly filled with Bio-Oss, Bone-Fill, Gen-Ox anorganic or a blood clot. Four animals were sacrificed after 8 weeks; 12 weeks later, the remaining four were sacrificed. The contents of the cylinders were removed, cut and stained with HE before they were evaluated with an optical microscope. The samples were submitted to histomorphometry for analysis.
The bone formation with Bio-Oss at 8 weeks was 8.43 mm(2); at 12 weeks, it was 9.32 mm(2). The bone formation with Bone-Fill at 8 weeks was 7.24 mm(2); at 12 weeks, it was 9.01 mm(2). The bone formation with Gen-Ox anorganic at 8 weeks was 2.78 mm(2); at 12 weeks, it was 3.02 mm(2). The bone formation with the blood clot at 8 weeks was 0.65 mm(2); at 12 weeks, it was 0.63 mm(2).
Following this model, Bone-Fill was comparable to Bio-Oss and superior to Gen-Ox and blood clot.
无机牛异种移植物在种植义齿学中作为骨替代物表现出最佳性能。Bio-Oss是世界上使用最广泛且研究最多的无机骨替代物。本文将两种无机牛骨替代物(Bone-Fill和Gen-Ox无机骨)与Bio-Oss进行比较。
将8只新西兰兔植入4个随机填充有Bio-Oss、Bone-Fill、Gen-Ox无机骨或血凝块的钛圆柱体。8周后处死4只动物;12周后,处死其余4只。取出圆柱体内容物,切割并进行苏木精-伊红染色,然后用光学显微镜进行评估。将样本进行组织形态计量学分析。
Bio-Oss在8周时的骨形成量为8.43平方毫米;在12周时,为9.32平方毫米。Bone-Fill在8周时的骨形成量为7.24平方毫米;在12周时,为9.01平方毫米。Gen-Ox无机骨在8周时的骨形成量为2.78平方毫米;在12周时,为3.02平方毫米。血凝块在8周时的骨形成量为0.65平方毫米;在12周时,为0.63平方毫米。
按照此模型,Bone-Fill与Bio-Oss相当,且优于Gen-Ox和血凝块。