Hoffman Allen H, Teng Zhongzhao, Zheng Jie, Wu Zheyang, Woodard Pamela K, Billiar Kristen L, Wang Liang, Tang Dalin
Mechanical Engineering Department, Worcester Polytechnic Institute, Worcester, MA 01609.
Mathematical Sciences Department, Worcester Polytechnic Institute, Worcester, MA 01609.
J Biomech Eng. 2017 Dec 1;139(12):1245011-6. doi: 10.1115/1.4037794.
Arteries can be considered as layered composite material. Experimental data on the stiffness of human atherosclerotic carotid arteries and their media and adventitia layers are very limited. This study used uniaxial tests to determine the stiffness (tangent modulus) of human carotid artery sections containing American Heart Association type II and III lesions. Axial and circumferential oriented adventitia, media, and full thickness specimens were prepared from six human carotid arteries (total tissue strips: 71). Each artery yielded 12 specimens with two specimens in each of the following six categories; axial full thickness, axial adventitia (AA), axial media (AM), circumferential full thickness, circumferential adventitia (CA), and circumferential media (CM). Uniaxial testing was performed using Inspec 2200 controlled by software developed using labview. The mean stiffness of the adventitia was 3570 ± 667 and 2960 ± 331 kPa in the axial and circumferential directions, respectively, while the corresponding values for the media were 1070 ± 186 and 1800 ± 384 kPa. The adventitia was significantly stiffer than the media in both the axial (p = 0.003) and circumferential (p = 0.010) directions. The stiffness of the full thickness specimens was nearly identical in the axial (1540 ± 186) and circumferential (1530 ± 389 kPa) directions. The differences in axial and circumferential stiffness of media and adventitia were not statistically significant.
动脉可被视为层状复合材料。关于人类动脉粥样硬化颈动脉及其中膜和外膜层刚度的实验数据非常有限。本研究采用单轴试验来测定含有美国心脏协会II型和III型病变的人类颈动脉切片的刚度(切线模量)。从6条人类颈动脉制备了轴向和周向取向的外膜、中膜和全层标本(总共71个组织条带)。每条动脉产生12个标本,在以下六个类别中各有两个标本:轴向全层、轴向外膜(AA)、轴向中膜(AM)、周向全层、周向外膜(CA)和周向中膜(CM)。使用由LabVIEW开发的软件控制的Inspec 2200进行单轴试验。外膜在轴向和周向方向的平均刚度分别为3570±667和2960±331 kPa,而中膜的相应值分别为1070±186和1800±384 kPa。外膜在轴向(p = 0.003)和周向(p = 0.010)方向均显著比中膜硬。全层标本在轴向(1540±186)和周向(1530±389 kPa)方向的刚度几乎相同。中膜和外膜在轴向和周向刚度上的差异无统计学意义。