The objectives of this study were to investigate in vitro BPA release from two common fiberglass fixed lingual canine-to-canine retainers and to compare these amounts with those released from a conventional multistranded stainless-steel orthodontic retainer.
Fifty-four recently extracted teeth were divided into groups of six teeth each, formed in an arch shape. Three different retainer types were evaluated: Ribbond, EverStick Ortho and Wildcut wire. Three identical specimens were constructed for each retainer type. BPA release was determined with validated the liquid chromatography-tandem mass spectrometry method at 1 and 24 h, as well as at 7, 14 and 30 days. The method's limits of detection and quantification were 0.32 ng/mL and 0.96 ng/mL, respectively. A two-way mixed, repeated-measures analysis of variance with Greenhouse-Geisser correction was employed to verify the existence of any significant differences.
Higher levels of BPA were released from the polyethylene fiber and glass fiber retainer in comparison with the conventional retainer in the present study. The differences between the systems over time were not statistically significant at the 95% confidence level.
In vitro BPA release during the first month did not differ between the examined retainer types. The highest BPA concentrations were observed at 1 month.
本研究的目的是调查两种常见的玻璃纤维固定舌侧犬齿至犬齿保持器在体外的双酚A(BPA)释放情况,并将这些释放量与传统多股不锈钢正畸保持器的释放量进行比较。
将54颗近期拔除的牙齿分成每组6颗牙齿的组,形成牙弓形状。评估三种不同类型的保持器:Ribbond、EverStick Ortho和Wildcut丝。每种保持器类型构建三个相同的标本。采用经过验证的液相色谱-串联质谱法在1小时和24小时以及7天、14天和30天时测定BPA释放量。该方法的检测限和定量限分别为0.32纳克/毫升和0.96纳克/毫升。采用带Greenhouse-Geisser校正的双向混合重复测量方差分析来验证是否存在任何显著差异。
在本研究中,与传统保持器相比,聚乙烯纤维和玻璃纤维保持器释放出更高水平的BPA。在95%置信水平下,不同系统随时间的差异无统计学意义。
在第一个月期间,所检查的保持器类型之间的体外BPA释放没有差异。在1个月时观察到最高的BPA浓度。