Department of Prosthetic Dentistry, Institute of Dentistry, University of Turku, Finland.
Acta Biomater. 2010 Oct;6(10):4136-42. doi: 10.1016/j.actbio.2010.05.017. Epub 2010 May 23.
This study has examined the use of polyvinylphosphonic acid (PVPA) as a potential matrix metalloproteinase (MMP) inhibitor and how brief cross-linking of demineralized dentin matrix that did not affect its mechanical properties enhanced the anti-MMP activity of PVPA. The anti-MMP potential of five PVPA concentrations (100-3000 microgml(-1)) was initially screened using a rhMMP-9 colorimetic assay. Demineralized dentin beams were treated with the same five concentrations of PVPA to collagen and then aged for 30 days in a calcium- and zinc-containing medium. The changes in modulus of elasticity, loss of dry mass and dissolution of collagen peptides were measured via three-point bending, precision weighing and hydroxyproline assay, respectively. All tested PVPA concentrations were highly effective (P<0.05) in inhibiting MMP-9. Ageing in the incubation medium did not significantly alter the modulus of elasticity of the five PVPA treatment groups. Conversely, aged dentin beams from the control group exhibited a significant decline in their modulus of elasticity (P<0.05) over time. Mass loss from the dentin beams and the corresponding increase in hydroxyproline in the medium in the five PVPA treatment groups were significantly lower than for the control (P<0.05). PVPA is a potent inhibitor of endogenous MMP activities in demineralized dentin. It may be used as an alternative to chlorhexidine to prevent collagen degradation within hybrid layers to extend the longevity of resin-dentin bonds.
本研究探讨了聚乙烯膦酸(PVPA)作为潜在基质金属蛋白酶(MMP)抑制剂的用途,以及对脱矿牙本质基质进行短暂交联而不影响其机械性能如何增强 PVPA 的抗 MMP 活性。最初使用 rhMMP-9 比色测定法筛选了五种 PVPA 浓度(100-3000μg/ml)的抗 MMP 潜力。用相同的五种浓度的 PVPA 处理脱矿牙本质梁以交联胶原,然后在含有钙和锌的培养基中老化 30 天。通过三点弯曲、精密称重和羟脯氨酸测定法分别测量弹性模量、干质量损失和胶原肽溶解的变化。所有测试的 PVPA 浓度均能有效(P<0.05)抑制 MMP-9。在孵育培养基中老化不会显著改变五种 PVPA 处理组的弹性模量。相反,对照组的老化牙本质梁的弹性模量随时间显著下降(P<0.05)。五组 PVPA 处理组的牙本质梁的质量损失和相应的介质中羟脯氨酸增加明显低于对照组(P<0.05)。PVPA 是脱矿牙本质中内源性 MMP 活性的有效抑制剂。它可以替代洗必泰,以防止混合层内的胶原降解,从而延长树脂-牙本质粘结的寿命。