Suppr超能文献

不同灭菌剂对种植修复中不同印模材料尺寸精度影响的评估——一项研究

Assessment of Effect of Different Sterilization Agents on Dimensional Accuracy of Different Impression Materials in Implant Prosthesis - An Study.

作者信息

Kavita Kumari, Reddy K R Parameshwar, Reddy K R Maheshwar, Kumar Swatantra, Pandey Gyanendra, Singh Revati

机构信息

Department of Dentistry, Nalanda Medical College and Hospital, Patna, Bihar, India.

Department of Oral and Maxillofacial Surgery, Malla Reddy Institute of Dental Sciences, Hyderabad, Telangana, India.

出版信息

J Pharm Bioallied Sci. 2021 Nov;13(Suppl 2):S1620-S1623. doi: 10.4103/jpbs.jpbs_315_21. Epub 2021 Nov 10.

Abstract

AIM

Sterilization of impression materials is of paramount importance. The present study was conducted to compare the effect of different disinfectants on dimensional accuracy of elastomeric impression materials used for implant prosthesis and other routine treatments.

MATERIALS AND METHODS

The present study was conducted with polyvinyl siloxane (PVS) (regular body), PVS (medium body), PVS (heavy body), and polyether (medium body) impression materials. Glutaraldehyde (2%) and sodium hypochlorite (NaOCl, 0.525%) were the disinfectant solutions employed in the study. After 16 h, the specimens were measured under Leica WILD stereomicroscope and dimensions were compared with master die.

RESULTS

The dimensional change in the Controls, 2% glutaraldehyde (Group I), and 0.525% NaOCl (Group II) was non significant where as Group III and Group IV showed statistically significant difference ( < 0.05). Results also showed significantly higher tear strength (newton/millimeter) in Control group followed by Group I and Group II.

CONCLUSION

PVS (heavy body) was found to be most stable, and polyether was seen to be stable of all the impression materials.

摘要

目的

印模材料的消毒至关重要。本研究旨在比较不同消毒剂对用于种植义齿及其他常规治疗的弹性印模材料尺寸精度的影响。

材料与方法

本研究采用了聚乙烯基硅氧烷(PVS)(常规型)、PVS(中型)、PVS(重型)和聚醚(中型)印模材料。研究中使用的消毒溶液为戊二醛(2%)和次氯酸钠(NaOCl,0.525%)。16小时后,在徕卡WILD立体显微镜下测量标本,并将尺寸与主模型进行比较。

结果

对照组、2%戊二醛组(I组)和0.525% NaOCl组(II组)的尺寸变化不显著,而III组和IV组显示出统计学上的显著差异(<0.05)。结果还显示,对照组的撕裂强度(牛顿/毫米)显著高于I组和II组。

结论

发现PVS(重型)在所有印模材料中最稳定,聚醚也较为稳定。

https://cdn.ncbi.nlm.nih.gov/pmc/blobs/e4d7/8686873/0704a756206d/JPBS-13-1620-g001.jpg

文献AI研究员

20分钟写一篇综述,助力文献阅读效率提升50倍。

立即体验

用中文搜PubMed

大模型驱动的PubMed中文搜索引擎

马上搜索

文档翻译

学术文献翻译模型,支持多种主流文档格式。

立即体验